[1]侯永利,杨爱民.前摆式螺旋焊管机组工艺及调型分析[J].焊管,2011,34(6):43-46.[doi:1001-3938(2011)06-0043-04]
 HOU Yong-li,YANG Ai-min.Front-swing Type Spiral Welded Pipe Unit Process and Forming Adjustment Analysis[J].,2011,34(6):43-46.[doi:1001-3938(2011)06-0043-04]
点击复制

前摆式螺旋焊管机组工艺及调型分析
分享到:

《焊管》[ISSN:1001-3938/CN:61-1160/TE]

卷:
34
期数:
2011年第6期
页码:
43-46
栏目:
工艺与设备
出版日期:
2011-06-28

文章信息/Info

Title:
Front-swing Type Spiral Welded Pipe Unit Process and Forming Adjustment Analysis
文章编号:
1001-3938(2011)06-0043-04
作者:
侯永利  杨爱民
1. 西安石油大学 材料科学与工程学院 西安 710065;
2.宝鸡石油钢管有限责任公司,陕西 宝鸡 721008
Author(s):
HOU Yong-li YANG Ai-min
1. School of Material Science and Engineering,Xi’an Shiyou University,Xi’an 710065,China;
 2.Baoji Petroleum Steel Pipe Co., Ltd., Baoji 721008, Shaanxi, China
关键词:
前摆式螺旋埋弧焊管机组调型成型稳定性
Keywords:
 front-swing typespiral welded pipe unitforming adjustmentforming stability
分类号:
TG335.75
DOI:
1001-3938(2011)06-0043-04
文献标志码:
B
摘要:
以某前摆式焊管机组为例,介绍了其工艺布置、成型器结构和原理及成型调型工艺参数。指出了机组成型的调型原则是:前桥的回转中心、焊垫辊的定位中心以及后桥中心线的垂直投影必须与滑台的中心线严格重合;前桥钢带的递送线要严格平行于前桥中心线, 后桥中心线必须平行于成型器底座的中心线;成型器内钢管的出管标高应与后桥扶正器、输出辊道等辅助设备的相关标高协调一致。最后探讨了前摆式螺旋埋弧焊管机组的成型稳定性。
Abstract:
Taking the front-swing type spiral welded pipe unit as an example, it introduced its process layout, structure and working principle of forming machine and forming adjustment parameters. It pointed out the adjusting principles are as following: the circumgyrating center of front bridge, positioning center of welding pad roller and the vertical projection of back bridge centerline will fully coincide with the centerline of slipway; the delivery line of front bridge strip should be parallel to front bridge centerline, back bridge centerline should be parallel to the centerline of forming machine base; the benchmark of pipe output in forming machine should be in accordance with the relevant benchmarks of auxiliary equipment, such as back bridge stabilizer, output roller and so on. Finally, it also discussed forming stability of front-swing type spiral welded pipe unit.

参考文献/References:

[1] 李鹤林.中国焊管50年[M].西安:陕西科学技术出版社,2008.
[2] 黄志潜. 黄志潜文集(第一卷),油气输送管道用螺旋埋弧焊接钢管的制造技术[M].西安:陕西科学技术出版社,2006.
[3] 闫立学,李志强,陈其卫.前摆式螺旋焊管机组调型初探[J]. 焊管,2003,26(2):51-52.

相似文献/References:

[1]秦跃平.前摆式螺旋埋弧焊管机组内焊缝裂纹产生原因分析[J].焊管,2008,31(4):62.[doi:1001-3938(2008)04-0062-02]
 QIN Yue-ping.Analysis on Reason of Inside Weld Crack of Front Swing SSAW Pipe Units[J].,2008,31(6):62.[doi:1001-3938(2008)04-0062-02]
[2]王刚.前摆式螺旋埋弧焊管机组递送线的控制[J].焊管,2010,33(9):41.[doi:1001-3938(2010)09-0041-03]
 WANG Gang.Delivery Line Control of Front-swing Type SAWH Pipe Unit[J].,2010,33(6):41.[doi:1001-3938(2010)09-0041-03]

备注/Memo

备注/Memo:
作者简介:侯永利(1976—),男,西安石油大学在读工程硕士, 主要从事螺旋埋弧焊管生产工艺设计和研究工作。
更新日期/Last Update: