[1]李 东,尹立孟,王学军,等.管线钢焊缝中晶内针状铁素体的研究进展[J].焊管,2016,39(2):10-13,18.[doi:10.19291/j.cnki.1001-3938.2016.02.003]
 LI Dong,YIN Limeng,WANG Xuejun,et al.Research Progress of Intragranular Acicular Ferrite in Pipeline Steel Weld[J].,2016,39(2):10-13,18.[doi:10.19291/j.cnki.1001-3938.2016.02.003]
点击复制

管线钢焊缝中晶内针状铁素体的研究进展
分享到:

《焊管》[ISSN:1001-3938/CN:61-1160/TE]

卷:
39
期数:
2016年第2期
页码:
10-13,18
栏目:
试验与研究
出版日期:
2016-02-28

文章信息/Info

Title:
Research Progress of Intragranular Acicular Ferrite in Pipeline Steel Weld
文章编号:
10.19291/j.cnki.1001-3938.2016.02.003
作者:
李 东1尹立孟1王学军2蒋 勇3耿燕飞1姚宗湘1
1. 重庆科技学院冶金与材料工程学院, 重庆  401331;
2. 四川石油天然气建设工程有限责任公司, 成都 610041;
3. 四川大西洋焊接材料股份有限公司, 四川 自贡643000
Author(s):
LI Dong1 YIN Limeng1 WANG Xuejun2 JIANG Yong3 GENG Yanfei1 YAO Zongxiang1
1. School of Metallurgy and Materials Engineering, Chongqing University of Science and Technology, Chongqing 401331, China;
2. Sichuan Petroleum Construction Engineering Co., Ltd, Chengdu 610041, China;
3. Sichuan Atlantic Welding Consumable, Zigong 643000, Sichuan, China
关键词:
管线钢晶内形核针状铁素体(IAF)形核长大机理
Keywords:
pipeline steel intragranular acicular ferrite(IAF) nucleation growth mechansim
分类号:
TG113.12
DOI:
10.19291/j.cnki.1001-3938.2016.02.003
文献标志码:
A
摘要:
为了研究晶内针状铁素体(intragranular acicular ferrite, IAF)对低碳微合金高强度管线钢焊接质量的影响,从IAF的本质、形核机理和长大以及影响其形核的因素等几方面进行了详细分析。研究认为,IAF是一种以非金属夹杂物诱发形核长大的组织,夹杂物种类、夹杂物尺寸、原奥氏体晶粒尺寸和冷却速度是影响其形核的主要因素,低碳微合金高强度管线钢焊缝中的IAF具有显著提高管线钢强度和改善韧性的作用。研究结果以期为高性能管线钢焊接的深入研究及生产实践提供科学指导与参考。
Abstract:
In order to study the influence of intragranular acicular ferrite (IAF) on welding quality of low carbon microalloyed high strength pipeline steel, in this article, it detailedly analyzed from several aspects, such as IAF essence, nucleation mechanism and grow up, and effect factors on nucleation. The research results considered IAF is a kind of structure caused by non-metallic inclusion inducing nucleation, inclusions species, inclusions size, the original austenite grain size and cooling rate are the main factors affecting nucleation. IAF in low carbon microalloyed high strength pipeline steel weld can significantly improve the strength and toughness of pipeline steel. The study will provide scientific guidance and reference for further research and production practice of high performance pipeline steel welding.

参考文献/References:

[1] 严春妍,黄健成,田松亚,等. X80高Nb管线钢组织与性能分析[J]. 焊管,2013,36(7): 5-10.
[2] 高惠临. 管线钢与管线钢管[M]. 北京: 中国石化出版社,2012.
[3] 辛希贤,姚婷珍,张刊林,等. 高屈强比管线钢的安全性分析[J]. 焊管,2006,29(4): 36-39.
[4] 杨杰,李春福,申文竹. 针状铁素体形成的研究现状及应用前景[J]. 金属热处理,2013,38(2): 21-25.
[5] RICKS R A,HOWELL P R,BARRITTE G S. The nature of acicular ferrite in HSLA steel weld metals[J]. Journal of Materials Science,1982,17(3): 732-740.
[6] YANG J R,BHADESHIA H. Acicular ferrite transformation in alloy-steel weld metals[J]. Journal of Materials Science,1991,26(3): 839-845.
[7] GHOMASHCHI R,COSTIN W,KURJI R. Evolution of weld metal microstructure in shielded metal arc welding of X70 HSLA steel with cellulosic electrodes: A case study[J]. Materials Characterization,2015(107): 317-326.
[8] BABU S S. The Mechanism of acicular ferrite in weld deposits[J]. Current Opinion in Solid State and Materials Science,2004,8(3): 267-278.
[9] ZHANG S,HATTORI N,ENOMOTO M,et al. Ferrite nucleation at ceramic/austenite interfaces[J]. ISIJ International,1996,36(10): 1301-1309.
[10] 张国栋. 焊缝中的针状铁素体行为及其模拟[D]. 武汉:华中科技大学,2002.
[11] SHIM J H,BYUN J S,CHO Y W,et al. Mnabsorption characteristics of Ti2O3 inclusions in low carbon steels[J]. Scripta Materialia,2001,44(1): 49-54.
[12] 余圣甫,雷毅,谢明立,等. 晶内铁素体的形核机理[J]. 钢铁研究学报,2005,17(1): 47-50.
[13] 尚成嘉,王学敏,杨善武,等. 高强度低碳贝氏体钢工艺与组织细化[J]. 金属学报,2003,39(10): 1019-1024.
[14] 黄安国,赵永,周龙早,等. 针状铁素体焊缝金属二次热循环的析出行为[J]. 机械工程材料,2006(10): 73-76.
[15] KOSEKI T,THEWLIS G. Inclusion assisted microstructure control in C-Mn and low alloy steel welds[J]. Materials Science and Technology,2005,21(8): 867-879.
[16] WAN X,WANG H,CHENG L,et al. The Formation mechanisms of interlocked microstructures in low-carbon high-strength steel weld metals[J]. Materials Characterization,2012(67): 41-51.
[17] 黄安国,余圣甫,谢明立,等. 低合金钢焊缝的针状铁素体微观组织[J]. 焊接学报,2008,29(3): 45-48.
[18] 余圣甫,余阳春,谢明立,等. 二次热循环对晶内铁素体的影响[J]. 焊接学报,2003,24(2): 89-92.
[19] SUNG H K,SHIN S Y,CHA W,et al. Effects of acicular ferrite on charpyimpact properties in heat affected zones of oxide-containing API X80 linepipesteels[J]. Materials Science and EngineeringA,2011,528(9): 3350-3357.
[20] PARK K T,HWANG S W,JI J H,et al. Inclusions nu-cleating intragranular polygonal ferrite and acicular ferrite cleating intragranular polygonal ferrite and acicular ferrite in low alloyed carbon manganese steel welds[J].Metals and Materials International,2011,17(2): 349-356.
[21] WAN X, WU K, NUNE K C, et al. In situ observation of acicular ferrite formation and grainrefinement in simulated heat affected zone of high strength low alloy steel[J]. Science and Technology of Welding and Joining, 2015,20(3): 254-263.
[22] LEE T K, KIM H J, KANG B Y, et al. Effect of inclusion size on the nucleation of acicular ferrite in welds[J]. ISIJ International, 2000, 40(12): 1260-1268.
[23] SHI M, ZHANG P, ZHU F. Toughness and microstructure of coarse grain heat affected zone with high heat input welding in Zr-bearing low carbon steel[J]. ISIJ International, 2014, 54(1): 188-192.
[24] 余圣甫,王杰. 药芯焊丝焊缝中的夹杂物对针状铁素体形成的影响规律[J]. 应用科学学报, 2000, 18(3):192-197.

相似文献/References:

[1]李新华,罗金恒,赵新伟,等.高钢级管线钢失效评估曲线研究[J].焊管,2007,30(4):33.[doi:1001-3938(2007)04-0033-03]
 LI Xin-hua,LUO Jin-heng,ZHAO Xin-wei,et al.Research on Failure Assessment Curves of High Grade Pipeline Steel[J].,2007,30(2):33.[doi:1001-3938(2007)04-0033-03]
[2]宫少涛,王爱民,吉玲康,等.X80与X100级管线钢屈服强度Rt 0.5与Rp 0.2的差异性研究[J].焊管,2007,30(5):42.[doi:1001-3938(2007)05-0042-03]
 GONG Shao-tao,WANG Ai-min,JI Ling-kang,et al.Study on Difference Between Yield Strength Rt 0.5 and Rp 0.2 for X80 and X100 Pipelines Steel[J].,2007,30(2):42.[doi:1001-3938(2007)05-0042-03]
[3]刘庆才,李 东,黎剑锋.影响输气管线钢管抗H2S性能主要因素的探讨[J].焊管,2007,30(5):54.[doi:1001-3938(2007)05-0054-05]
 LIU Qing-cai,LI Dong,LI Jian-feng.Key Factors Affecting Sour Service Ability of Welded Pipe and Its Domestic Production[J].,2007,30(2):54.[doi:1001-3938(2007)05-0054-05]
[4]王树人,崔志新.管线钢落锤撕裂试验异常脆性断口分析[J].焊管,2007,30(6):69.[doi:1001-3938(2007)06-0069-03]
 WANG Shu-ren? CUI Zhi-xin.Analysis on Abnormal Brittle Fracture of DWTT for Pipeline Steel[J].,2007,30(2):69.[doi:1001-3938(2007)06-0069-03]
[5]陶 鹏,张 弛,杨志刚,等.高钢级管线钢的组织和力学性能[J].焊管,2008,31(2):19.[doi:1001-3938(2008)02-0019-04]
 TAO Peng,ZHANG Chi,YANG Zhi-gang,et al.The Microstructure and Mechanical Property of X70,X80 and X100 Grade Pipeline Steel[J].,2008,31(2):19.[doi:1001-3938(2008)02-0019-04]
[6]黄明浩,徐 烽,黄国建.影响管线钢屈强比的因素探讨[J].焊管,2008,31(3):20.[doi:1001-3938(2008)03-0020-04]
 HUANG Ming-hao,XU Feng,HUANG Guo-jian.Discussion on Influencing Factors of Yield Ratio for Pipeline Steel[J].,2008,31(2):20.[doi:1001-3938(2008)03-0020-04]
[7]牛 辉,余大涛,高惠临.管线钢焊接热影响区的组织预测[J].焊管,2008,31(3):28.[doi:1001-3938(2008)03-0028-05]
 NU Hui,YU Da-tao,GAO Hui-lin.Structure Forecast of Pipeline Steel Welding Heat Affected Zone[J].,2008,31(2):28.[doi:1001-3938(2008)03-0028-05]
[8]孔君华,郑 琳,关 云,等.西气东输二线工程用18.4 mm厚 X80级热轧板卷生产实践[J].焊管,2008,31(6):50.[doi:1001-3938(2008)06-0050-04]
 KONG Jun-hua,ZHENG Ling,GUAN Yun,et al.Production Experience of X80 Grade Hot Rolled Coil with 18.4 mm Thickness Used〖JZ〗for the Second West to East Gas Pipeline Project[J].,2008,31(2):50.[doi:1001-3938(2008)06-0050-04]
[9]黄国建,张英慧,孔祥磊,等.特厚规格X70和X80级热轧卷板的开发与应用[J].焊管,2009,32(2):17.[doi:1001-3938(2009)02-0017-06]
 HUANG Guo-jian,ZHANG Ying-hui,KONG Xiang-lei,et al.Development and Application of X70 & X80 Grade HRC with Heavy Thickness[J].,2009,32(2):17.[doi:1001-3938(2009)02-0017-06]
[10]杨专钊,李云龙,邓波,等.管线钢拉伸试验中异常屈服强度研究与分析[J].焊管,2009,32(4):51.[doi:1001-3938(2009)04-0051-03]
 YANG Zhuan-zhao,LI Yun-long,DENG Bo,et al.Research and Analysis of Abnormal Yield Strength during Tensile Test of Pipeline Steel[J].,2009,32(2):51.[doi:1001-3938(2009)04-0051-03]

备注/Memo

备注/Memo:
收稿日期: 2015-11-30
基金项目: 重庆市前沿与应用基础研究项目(cstc2014 jcyjA40009、 cstc2015jcyjA50017), 重庆市研究生科研创新项目(CYS15227)。
作者简介: 李   东(1992—), 男, 硕士研究生, 主要从事高性能管线钢焊接与力学可靠性评价工作。