[1]田永吉,苏 琬,王宝宝.SEW J55 钢级LC套管螺纹连接质量影响因素探讨[J].焊管,2020,43(8):30-37.[doi:10.19291/j.cnki.1001-3938.2020.08.006]
 TIAN Yongji,SU Wan,WANG Baobao.Discussion on Influencing Factors of SEW J55 LC Casing Thread Connection Quality[J].,2020,43(8):30-37.[doi:10.19291/j.cnki.1001-3938.2020.08.006]
点击复制

SEW J55 钢级LC套管螺纹连接质量影响因素探讨()
分享到:

《焊管》[ISSN:1001-3938/CN:61-1160/TE]

卷:
43
期数:
2020年第8期
页码:
30-37
栏目:
应用与开发
出版日期:
2020-08-28

文章信息/Info

Title:
Discussion on Influencing Factors of SEW J55
LC Casing Thread Connection Quality
文章编号:
10.19291/j.cnki.1001-3938.2020.08.006
作者:
田永吉苏 琬王宝宝
宝鸡钢管西安石油专用管公司, 陕西 宝鸡 721008
Author(s):
TIAN Yongji SU Wan WANG Baobao
Xi’an OCTG Company of BSG Group, Baoji 721008, Shaanxi, China
关键词:
SEWLC套管螺纹拧接扭矩
Keywords:
SEWLC casingthreadscrew on torque
分类号:
TE931.2
DOI:
10.19291/j.cnki.1001-3938.2020.08.006
文献标志码:
B
摘要:
为了进一步分析SEW J55 LC套管螺纹连接质量的影响因素以及套管发生异常脱扣失效的原因,以Φ139.7 mm×7.72 mm SEW J55 LC套管为例,从套管使用工况、螺纹加工参数、拧接扭矩控制等方面进行了试验研究。结果显示,SEW套管在弯曲状态拉脱试验、螺纹参数极限匹配下拉脱试验的拉脱载荷均高于API TR 5C3标准要求。研究表明,按照内控标准生产加工的SEW套管满足标准要求,弯曲工况、螺纹加工工艺、存放时间和J值均不是套管异常脱扣失效的原因。为提升SEW J55 LC套管螺纹连接质量,预防套管在油田使用中出现异常反拧退扣,建议将拧接扭矩在推荐标准基础上增大10%执行。
Abstract:
In order to further analyze the influencing factors of thread connection quality of SEW J55 LC casing and the cause of abnormal tripping failure of casing, taking Φ139.7 mm × 7.72 mm SEW J55 LC casing as an example, the test research is carried out from the aspects of casing service conditions, thread processing parameters and screw torque control. The results show that the pull-out load of SEW casing in bending state and thread parameter limit matching pull-out test are higher than the requirements of API TR 5C3 standard. The study indicate that the SEW casing produced and processed according to the internal control standard meets the requirements of the standard, and the bending condition, thread processing technology, storage time and J value are not the causes of casing abnormal tripping failure. In order to improve the quality of SEW J55 LC casing thread connection and prevent abnormal reverse screwing and thread withdrawal during casing application in oilfield, it is recommended to increase the screw-on torque by 10% on the basis of the recommended standard.

参考文献/References:

[1] API SPEC 5CT—2011,美国石油学会标准套管和油管规范(第9版)[S].
[2] API SPEC 5B—2017,套管、油管和管线管螺纹的加工、测量和检验规范(第16版)[S].
[3] ISO 13679:2002,石油和天然气工业—管道连接试验程序[S].
[4] API TR 5C3—2018,套管或油管的性能计算(第7版)[S].
[5] API RP 5C1—1999,套管和油管的维护及使用(第18版)[S].
[6] GB/T 17745—1999,石油天然气工业套管和油管的维护及使用[S].
[7] 宋治,冯耀荣. 油井管与管柱技术及应用[M]. 北京:石油工业出版社,2007.
[8] 卫遵义,吉玲康,董秋莹,等. API圆螺纹套管及接箍螺纹紧密距释疑[J]. 石油机械,1999,27(10):35-37.
[9] 艾裕丰,吴健,卫尊义,等. API油管和套管螺纹加工与检测探讨[J]. 焊管,2013,35(5):45-49.
[10] 王一岑,苑青英,符利兵,等. 油套管上卸扣扭矩准确度的影响因素及改善措施[J]. 焊管,2017,40(1):54-58.
[11] 罗华权,杨力能,何小东,等. 油田压裂弯头失效控制及检测评价[J]. 石油工业技术监督,2018,34(3):1-6.
[12] 宋明哲,单锋,卢俊安,等. 塔里木高温高压气井套管头堵漏技术研究与应用[J]. 石油工业技术监督,2018,34(2):4-5.

相似文献/References:

[1]田永吉,李跟社,苏 琬,等.J55钢级SEW管坯调质生产N80Q套管工艺研究[J].焊管,2018,41(4):46.[doi:10.19291/j.cnki.1001-3938.2018.04.010]
 TIAN Yongji,LI Genshe,SU Wan,et al.Process Research on J55 Steel Grade(TG22) SEW Tube Blank Quenching and Tempering Production N80Q Casing[J].,2018,41(8):46.[doi:10.19291/j.cnki.1001-3938.2018.04.010]

备注/Memo

备注/Memo:
收稿日期:2020-02-10
作者简介:田永吉(1984—),男,工学学士,工程师,现主要从事石油专用管生产质量管理工作。
更新日期/Last Update: 2020-09-16