[1]王涛,任永峰,雒设计.HFW焊管沟槽腐蚀研究现状[J].焊管,2022,45(8):1-9.[doi:10.1929 1/j.cnki.1001-3938.2022.08.001]
 WANG Tao,REN Yongfeng,LUO Sheji.Research Status of Groove Corrosion of HFW Welded Pipe[J].,2022,45(8):1-9.[doi:10.1929 1/j.cnki.1001-3938.2022.08.001]
点击复制

HFW焊管沟槽腐蚀研究现状()
分享到:

《焊管》[ISSN:1001-3938/CN:61-1160/TE]

卷:
45
期数:
2022年第8期
页码:
1-9
栏目:
综述
出版日期:
2022-08-28

文章信息/Info

Title:
Research Status of Groove Corrosion of HFW Welded Pipe
文章编号:
10.1929 1/j.cnki.1001-3938.2022.08.001
作者:
王涛任永峰雒设计
1.国家石油天然气管材工程技术研究中心,陕西 宝鸡 721008;2.宝鸡石油钢管有限责任公司,陕西 宝鸡 721008; 3.西安石油大学,西安 710065
Author(s):
WANG TaoREN YongfengLUO Sheji
1. Chinese National Engineering Research Center for Petroleum and Natural Gas Tubular Goods,Baoji 721008,Shaanxi,China;2. Baoji Petroleum Steel Pipe Co,Ltd.,Baoji 721008,Shaanxci,China;3. Xi’an Shiyou University,Xi’ an 710065,China
关键词:
HFW焊管沟槽腐蚀敏感系数影响因素测试方法
Keywords:
HFW welded pipegroove corrosionsensitivity coefficientinfluence factortest method
分类号:
TG174
DOI:
10.1929 1/j.cnki.1001-3938.2022.08.001
文献标志码:
A
摘要:
为充分了解HFW焊管焊缝沟槽腐蚀机理,及其对高频电阻焊管力学性能的影响,从而探索出有效降低HFW焊管沟槽腐蚀敏感性的方法,从沟槽腐蚀影响规律、测试方法等方面对国内外现阶段沟槽腐蚀研究成果进行分析汇总,着重分析了几种主要的沟槽腐蚀敏感性测试方法,对其优劣性进行了对比。同时,根据沟槽腐蚀研究现状以及相关知识产权的情况,发现目前国内外尚无统一标准的焊缝沟槽腐蚀深度的测量设备或装置,对沟槽腐蚀敏感系数临界值也缺乏工程依据,其失效判定的有效性有待进一步探讨。
Abstract:
In order to fully understand the mechanism of HFW welded pipe weld groove corrosion and its influence on the mechanical properties of resistance welded pipe,and explore the methods to effctively reduce the groove corrosion sensitivity of welded pipe,the research results of groove corrosion at home and abroad at this stage are analyzed and summarized from the aspects of groove corrosion impact law,testing methods and so on. Several main groove corrosion sensitivity test methods are emphatically analyzed,and their advantages and disadvantages are compared. At the same time,according to the research status of groove corrosion and relevant intellectual property rights,it is found that there is no unified standard equipment or device for measuring the groove corrosion depth of weld at home and abroad, and there is also a lack of engineering cases for the critical value of groove corrosion sensitivity coefficient,and the effectiveness of its failure determination needs to be further discussed.

参考文献/References:

[1]王荣.显微组织和热处理对直缝电阻焊管沟槽腐蚀的影响[J].金属学报,2002,38(12):6-10.[2]毕宗岳,井晓天,鲜林云,等.热处理对连续油管焊缝沟槽腐蚀行为的影响[J].热加工工艺,2011,40(8):4-7.[3] WANGR,BIZ Y,JING X T. Grooving corrosion of oil coiled tubes manufactured by electrical resistance welding[J]. Corrosion Science,2012(5):67-73.[4]王荣.J55钢直缝焊油井套管沟槽腐蚀性能研究[J].中国腐蚀与防护学报,2004,24(6):4-10.[5] WANG R. Grooving corrosion properties of electric resistance welded oil well casing of J55 steel[J]. Journal of the Chinese Society of Corrosion and Protection,2004,24(6):360- 363. [6] KATO C,OTOGURO Y,KAD O S,et al. Grooving Corrosion in eletric resistance welded steel pipe in sea water[J].Corrosion Science,1978,18(1):61-74.[7] KURIS K T,HARADA S. Effect of various factors mechanisms and preventive method of grooving corrosion of HFW and CBW carbon steel pipes[J]. Kawasaki Steel Technical Report, 1979,11(3):321-336.[8] MASAMURA K,MATSUSHIMA I. Case studies of grooving corrosion of electric resistance welded pipe[J]. Corrosion Engineering,1982,17(1):27-33.[9] HARA T,UEMORI R,TAMEHIRO H,et al. Mechanism of grooving corrosion resistance in Cu-Ti added high frequency electric resistance welded steel pipes[J]. Zairyo-to-Kankyo,2000, 49(3):150- 158.[10] EI-SAYED M H. Grooving corrosion of seam welded oil pipelines[J].Case Studies in Engineering Failure Analysis,2014,14(5):36-42.[11] LYU C L,CAO W M,CHEN H,et al. Effects of residual tensile stress on grooving corrosion of ERW pipes [J].Corrosion and Protection,2010,31(7):512-514.[12]贺飞,尚成嘉,张峰,等.热张力减径对电阻焊油井套管沟槽腐蚀性能的影响[J].腐蚀与防护,2012,33(10):4-9.[13] 吕春雷,曹为民,陈浩,等.应力对直缝高频电阻焊管沟槽腐蚀的影响[J].腐蚀与防护, 2010(7):3-6.[14] 毕宗岳,刘道新,李轩,等.热处理对ERW焊缝沟槽腐蚀敏感行为的影响[J].材料热处理学报,2011,32(2):7-11.[15] MUELLER R A. Pitting and crevice corrosion in ERW carbon steel heat exchanger tubes[J]. Journal of Materials for Energy Systems,1980,2(2):17-22.[16]陈圣乾,赵大伟,张炜强,等.某油田井口输油管线焊缝腐蚀失效分析[J].腐蚀与防护,2012,33(10):4-7.[17]罗逸.天然气井油管腐蚀沟槽的形成原因[J]天然气工业,2002,22(1):3-8.[18] KATO C,OTOGURO Y,KADO S. Effect of alloying elements on grooving corrosion resistance of ERW steel pipe[J]. Zairyo-to-Kankyo,2009,23(9):425-432.[19] CELAL,DURAN E,TREISS G,et al. The resistance of high frequency inductive welded pipe to grooving corrosion in salt water[J]. Materials Performance,1986,17(5):43-51.[20] WANG W,LIU C S,ZHOU Q J,et al. Methods for assessing the grooving corrosion of high-frequency electric resistance welded pipes[J]. Baosteel Technical Research,2010(4):27-32. [21] WANG W,QI H B,LIU C,et al. Methods for assessing the grooving corrosion of high-frequency electric resistance welded pipes[J]. Baosteel Technical Research,2010(3):27-31.[22] LEWIS R E,HASSELLJ C,CHOI H J,et al. Qualifying ERW tubular products for sweet petroleum production environments[C].NACE International Annual Conference & Exposition. San Diego,US:NACE,1998:3-8.[23] VORUGANTI V S,LUFT H B,GEER D D,et al. Scanning reference electrode technique for the investigation of preferential corrosion of weldments in offshore applications[J]. Corrosion, 1991,47(5):343-351.[24]毕宗岳,任永峰,井晓天.微电极扫描法对HFW焊缝沟槽腐蚀敏感性研究[J].焊管,2011, 34(10):4-10.[25]印仁和,陈浩,曹为民,等. K55钢高频电阻焊管沟槽腐蚀性能研究[C]/第十四次全国电化学会议论文汇编.扬州:中国化学会,2007:632-633.[26] 魏华,王秀通, 高荣杰,等. SML、ERW管线钢在海泥中的腐蚀行为[J].电化学,2005,11(3):5-7.[27]邬中华.X52直缝焊管沟槽腐蚀评价方法的研究[J].太钢科技,2009(3):5-10.[28] KATOH K,KOSUGE N,ITOH S,et al. Evaluation of grooving corrosion-resistant high frequency electric resistance welded (HF-ERW) steel pipes by new electrochemical technique[J]. Nippon Steel Technical Repot,1989,11(5):5-7.[29] MASAMURA K,MATSUSHIMA I. Case studies of grooving corrosion of electric resistance welded pipe[J].Corrosion Engineering,1982,31(5):332-335.[30] DURAN C,TRIESS E, HERBSLEB G. The resistance of high frequency inductive welded pipe to grooving corrosion in salt water [J]. Mater. Performance (United States),1986,25(9):28-34.[31] 赵西岐,张骁勇,苑清英,等.新型N80焊管耐蚀性能研究[J].全面腐蚀控制,2017,31(12):6-11.[32]张志升,杜素珍,尹志福. J55钢级电阻焊(ERW)套管的焊缝沟槽腐蚀行为[J].腐蚀与防护,2019,40(5):323-327.[33]石荣满,刘书国. ERW钢管的沟槽腐蚀及结果分析[J].防腐保温技术,2004,12(4):6-12.[34]田青超,董晓明,丁维军.抗沟槽腐蚀高强度ERW焊接套管用钢、套管及生产方法:2007 10093967.9[P].2011-07-20.[35]王炜,齐慧滨,钱余海,等.一种采用外加恒电流快速评价焊管沟槽腐蚀敏感性的方法:200810201900.7[P].2010-06-09.[36]齐慧滨,王炜,钱余海,等.一种用微区腐蚀电流密度测量焊管沟槽腐蚀敏感性的方法:200910197594.9[P].2011-05-04.[37]王炜,齐慧滨,钱余海,等.一种用恒电位电解法测量焊管沟槽腐蚀的方法:200910197657.0[P]. 2011-05-04.[38]龚育才,陈戈,王震.一种焊管焊缝区沟槽腐蚀深度测量装置:201020170602.9[P].2010-12-29.[39]王炜,陈红星,钱余海,等.焊管沟槽腐蚀敏感性测试装置:201120080395.2[P]. 2011-11-23.

相似文献/References:

[1]张 喆,周月明,白云峰,等.HFW中频热处理线圈结构对加热效果的影响[J].焊管,2009,32(1):41.[doi:1001-3938(2009)01-0041-05]
 ZHANG Zhe,ZHOU Yue-ming,BAI Yun-feng,et al.Loop Structure of HFW Intermediate Frequency Heating Treatment Effect to Heating[J].,2009,32(8):41.[doi:1001-3938(2009)01-0041-05]
[2]季晓鹏,张浩,马会文.国内外大中直径HFW焊管工艺发展研究[J].焊管,2009,32(8):10.[doi:1001-3938(2009)08-0010-06]
 JI Xiao-peng,ZHANG Hao,MA Hui-wen.Discussion on the Development and Research of the Technology of Large Diameter Hi-quality HFW Pipe in Abroad and Domestic[J].,2009,32(8):10.[doi:1001-3938(2009)08-0010-06]
[3]王涛.HFW焊管生产N80Q、P110级套管和油管的工艺开发[J].焊管,2009,32(9):35.[doi:1001-3938(2009)09-0035-03]
 WANG Tao.Process Development of HFW N80Q,P110 Grade Casing and Tubing[J].,2009,32(8):35.[doi:1001-3938(2009)09-0035-03]
[4]邵毅.ERW钢管内毛刺清除设备分析[J].焊管,2009,32(9):44.[doi:1001-3938(2009)09-0044-03]
 SHAO Yi.Inside Burrs Clearing Equipment Analysis of HFW Steel Pipe[J].,2009,32(8):44.[doi:1001-3938(2009)09-0044-03]
[5]邵毅.HFW焊管内毛刺清除刀具的选用[J].焊管,2009,32(12):40.[doi:1001-3938(2009)12-0040-03]
 SHAO Yi.Inside Burr Elimination Scraper Selection for HFW Pipe[J].,2009,32(8):40.[doi:1001-3938(2009)12-0040-03]
[6]孙凤龙,戴学余,周玉林,等.宝钢HFW焊管生产线去内毛刺刀杆研制[J].焊管,2010,33(1):37.[doi:1001-3938(2010)01-0037-04]
 SUN Feng-long,DAI Xue-yu,ZHOU Yu-lin,et al.Development of Scraper Bar for Burr Wiped off of HFW Pipe Line of Baosteel[J].,2010,33(8):37.[doi:1001-3938(2010)01-0037-04]
[7]彭在美.从国产连续油管成功研制看我国焊管产品结构调整[J].焊管,2010,33(4):5.[doi:1001-3938(2010)04-0005-05]
 PENG Zai-mei.Analyzing Structure Adjustment of China Welded Pipe Product from Successful Trial-production of Domestic Coiled Tubing[J].,2010,33(8):5.[doi:1001-3938(2010)04-0005-05]
[8]肖国章,高霞,李六五.带钢质量对ERW焊管质量的影响[J].焊管,2010,33(4):55.[doi:1001-3938(2010)04-0055-03]
 XIAO Guo-zhang,GAO Xia,LI Liu-wu.The Quality Of ERW Pipe Impacted By Strip Quality[J].,2010,33(8):55.[doi:1001-3938(2010)04-0055-03]
[9]张永,马东利.HFW焊管生产线乳化液回收泵站的改进[J].焊管,2010,33(6):45.[doi:1001-3938(2010)06-0045-02]
 ZHANG Yong,MA Dong-li.Emulsion Recycling Pump Station Alteration of HFW Production Line[J].,2010,33(8):45.[doi:1001-3938(2010)06-0045-02]
[10]赖兴涛,崔俊.HFW焊管制管各工序质量控制[J].焊管,2010,33(10):60.[doi:1001-3938(2010)10-0060-05]
 LAI Xing-tao,CUI Jun.Quality Control of HFW Pipe Each Procedure During Production[J].,2010,33(8):60.[doi:1001-3938(2010)10-0060-05]
[11]毕宗岳,任永峰,井晓天.微电极扫描法对ERW焊缝沟槽腐蚀敏感性研究[J].焊管,2011,34(10):5.[doi:1001-3938(2011)10-0005-04]
 BI Zong-yue,REN Yong-feng,JING Xiao-tian.Study on HFW Weld Groove Corrosion Sensitivity by Microelectrode Scanning Method[J].,2011,34(8):5.[doi:1001-3938(2011)10-0005-04]
[12]王 涛,任永峰,何石磊,等.不同热处理工艺对HFW焊管沟槽腐蚀的影响[J].焊管,2016,39(6):18.[doi:10.19291/j.cnki.1001-3938.2016.06.004]
 WANG Tao,REN Yongfeng,HE Shilei,et al.Effect of Different Heat Treatment Technology on Grooving Corrosion of HFW Pipes[J].,2016,39(8):18.[doi:10.19291/j.cnki.1001-3938.2016.06.004]

备注/Memo

备注/Memo:
收稿日期:2022-01-08作者简介:王涛(1982—),男,高级工程师,主要从事油气管材耐腐蚀性能研究工作。基金项目:中国石油天然气股份有限公司科学研究与技术开发项目“超临界二 氧化碳长距离管道关键技术研究”(项目编号2021ZZ01)。