[1]柏明卓,郑 磊,张 备,等.基于应变设计用X70大直径UOE管线管的研发[J].焊管,2015,38(1):21-27.[doi:1001-3938(2015)01-0021-07]
 BAI Mingzhuo,ZHENG Lei,ZHANG Bei,et al.Research and Development of X70 Large Diameter UOE Line Pipefor Strain-based Design Application[J].,2015,38(1):21-27.[doi:1001-3938(2015)01-0021-07]
点击复制

基于应变设计用X70大直径UOE管线管的研发
分享到:

《焊管》[ISSN:1001-3938/CN:61-1160/TE]

卷:
38
期数:
2015年第1期
页码:
21-27
栏目:
试验与研究
出版日期:
2015-01-28

文章信息/Info

Title:
Research and Development of X70 Large Diameter UOE Line Pipe
for Strain-based Design Application
文章编号:
1001-3938(2015)01-0021-07
作者:
柏明卓1郑 磊1张 备2许海生3
(1. 上海宝钢中央研究院,上海 201900;
2. 上海宝钢股份有限公司制造管理部,上海 201900;
3. 上海宝钢股份有限公司钢管条钢事业部,上海 201900)
Author(s):
BAI Mingzhuo1 ZHENG Lei1 ZHANG Bei2 XU Haisheng3 
(1.Research Institute of Baoshan Iron & Steel Co., Ltd., Shangshai 201900, China;
2. Manufacturing and Management Department of Baoshan Iron & Steel Co., Ltd., Shangshai 201900, China;
3. Tube, Pipe and Bar Business Unit, Baoshan Iron & Steel Co., Ltd., Shangshai 201900, China)
关键词:
焊管基于应变设计X70管线管抗大变形应变时效双相组织
Keywords:
welded pipe strain-based design X70 line pipe high deformability strain aging dual phase microstructure
分类号:
TE973
DOI:
1001-3938(2015)01-0021-07
文献标志码:
A
摘要:
研究了不同轧钢工艺钢的不同微观组织以及这些微观组织对管线钢抗大变形性能的影响。筛选出抗大应变管线钢优选的组织设计,并基于铁素体+贝氏体的双相组织设计,生产了具有低屈强比、高均匀延伸率、高抗应变时效性能的X70 UOE管线管,实现1 016 mm×17.5 mm和1 016 mm×21.0 mm规格UOE焊管的工业化生产。通过工业化生产数据,分析了板、管及时效后性能的变化规律,并研究了时效温度和时效时间对抗应变性能的影响。
Abstract:
In this article, it studied the different microstructure of steel which obtained by different rolling process, as well as the influence of microstructure on high deformability performance. So the preferred microstructure for the high deformability pipeline steel was obtained. Based on ferrite + bainite dual phase microstructure, the X70 UOE line pipes with low YT ratio, high uniform elongation and High strain aging performance were produced, which realized industrial production for UOE pipe with size of ?准1 016 mm×17.5 mm and ?准1 016 mm×21.0 mm. Through industrial production data, it analyzed the performance change rule of plate, pipe and aging, and studied the influence of aging temperature and aging time on the strain resistance performance.

参考文献/References:

[1]SUZUKI N,TOYODA M. Seismic loading on buried pipelines and deformability of high strength linepipes[C]∥Proceedings of International Conference on the Application and Evaluation of High-grade Linepipes in Hostile Environments,Yokohama,Japan:[s.n.],2002:601-628.
[2]GLOVER A. Application of grade 550(X80) and grade 690(X100) in arctic climates[C]∥Proceedings of the International Pipe Dreamer’s Conference,Yokohama,Japan:[s.n.],2002:33-52.
[3]YATABE H,FUKUDA N,MASUDA T,et al. Application of X80 in Japan:earthquake resistance[C]∥Proceedings of the 4th International Pipeline Technology Conference,Ostend,Belgium:[s.n.],2004:1377-1396.
[4]李鹤林,李霄,吉玲康. 油气管道基于应变的设计及抗大变形管线钢的开发与应用[J]. 焊管,2007,30(05):5-11.
[5]GLOVER A,ROTHWELL B. Yield strength and plasticity of high strength pipelines[C]∥Proceedings of the 4th International Pipeline Technology Conference,Ostend,Belgium:[s.n.],2004:65-79.
[6]OKATSU M,SHINMIYA T,ISHIKAWA N,et al. Development of high strength linepipe with excellent deformability[C]∥24th International Conference on Off-shore Mechanics and Arctic Engineering,OMAE2005-67149,Halkidiki,Greece:ASME,2005.
[7]ISHIKAWA N,OKATSU M,ENDO S. High deformability UOE linepipes produced by advanced TMCP Technology[C] ∥ TMS eds. Proceedins of International Symposium on Microalloyed Steels for Oil & Gas Industry,Brazil:Araxa-MG,2006.
[8]SHIOHARA Y,HARA T,TSURU E,et al. Change of mechanical properties of high strength line pipe by themal coating yreatment[C]∥24th International Conference on Offshore Mechanics and Arctic Engineering,OMAE2005-67055,Halkidiki,Greece:ASME,2005.
[9] 崔天成,郑磊,吴海凤. 应变时效对不同成分高强度管线钢力学性能的影响[J]. 机械工程材料,2010,34(05):30-32.
[10]DUAN D M,ZHOU J,BRIAN R,et a1. Strain aging effects in high strength linePipe materials[C] ∥ Proceedings of IPC2008 7th International Pipeline Conference. Calgary:IPC,2008.
[11]Q/SY GJX 115—2011,中缅天然气管道基于应变设计地区直缝埋弧焊管技术条件(国内段)[S].

相似文献/References:

[1]马海君.强力焊管的孔型设计[J].焊管,2007,30(4):56.[doi:1001-3938(2007)04-0056-02]
 MA Hai-jun.Pass Design of High-strength Welded Pipe[J].,2007,30(1):56.[doi:1001-3938(2007)04-0056-02]
[2]刘庆才,李 东,黎剑锋.影响输气管线钢管抗H2S性能主要因素的探讨[J].焊管,2007,30(5):54.[doi:1001-3938(2007)05-0054-05]
 LIU Qing-cai,LI Dong,LI Jian-feng.Key Factors Affecting Sour Service Ability of Welded Pipe and Its Domestic Production[J].,2007,30(1):54.[doi:1001-3938(2007)05-0054-05]
[3]张 华,赵新伟,罗金恒,等.基于灰色关联度法的管道临界屈曲应变影响因素分析[J].焊管,2008,31(2):77.[doi:1001-3938(2008)02-0077-05]
 ZHANG Hua,ZHAO Xin-wei,LUO Jin-heng,et al.Discussion of the Influencing Factor on the Critical Buckling Strain for Pipelines Based on Gray Correlation Analysis[J].,2008,31(1):77.[doi:1001-3938(2008)02-0077-05]
[4]彭在美.我国焊接钢管的发展进入重要的战略转折期[J].焊管,2008,31(6):5.[doi:1001-3938(2008)06-0005-10]
 PENG Zai-mei.The Development of China Welded Pipe Steps into the Important Strategic Transition Period[J].,2008,31(1):5.[doi:1001-3938(2008)06-0005-10]
[5]李霄,熊庆人,石凯,等.焊管残余应力研究进展及展望[J].焊管,2009,32(7):12.[doi:1001-3938(2009)07-0012-06]
 LI Xiao,XIONG Qing-ren,SHI Kai,et al.Research Progress and Prospect of Residual Stress in Welded Pipe[J].,2009,32(1):12.[doi:1001-3938(2009)07-0012-06]
[6]马 露 涛.φ720mm焊管平头机夹管装置设计[J].焊管,2009,32(9):47.[doi:1001-3938(2009)09-0047-03]
 MA Lu-tao.Design for φ720mm Welded Pipe Beveling Machine Clamp Pipe Device[J].,2009,32(1):47.[doi:1001-3938(2009)09-0047-03]
[7]耿开博.铝管、不锈钢管的高频感应焊接[J].焊管,2009,32(11):29.[doi:1001-3938(2009)11-0029-03]
 GENG Kai-bo.High-frequency Induction Welding of Aluminum and Stainless Steel Pipes[J].,2009,32(1):29.[doi:1001-3938(2009)11-0029-03]
[8]陈志翔,Jean Paul Boillot,Jeff Noruk.数字激光视觉技术在焊管生产中的应用[J].焊管,2010,33(2):29.[doi:1001-3938(2010)02-0029-04]
 CHEN Zhi-xiang,Jean Paul Boillot,Jeff Noruk.Application of Digital Laser Vision Technology in Welded Pipe Production[J].,2010,33(1):29.[doi:1001-3938(2010)02-0029-04]
[9]马小芳,谢文江.输送管线基于应变的设计方法在我国的前景与展望[J].焊管,2010,33(4):62.[doi:1001-3938(2010)04-0062-04]
 MA Xiao-fang,XIE Wen-jiang.The Prospect of Transfer Pipeline Based on Strain Design in China[J].,2010,33(1):62.[doi:1001-3938(2010)04-0062-04]
[10]黄克坚,苏章卓,甘遂谋,等.焊管机械扩径力的计算[J].焊管,2010,33(12):13.[doi:1001-3938(2010)12-0023-04]
[11]王 旭,罗 超,陈小伟,等.我国抗大变形管线管的研制进展[J].焊管,2013,36(6):5.[doi:1001-3938(2013)06-0005-07]
 WANG Xu,LUO Chao,CHEN Xiaowei,et al.Development Progress of China Domestic High-deformability Line Pipe[J].,2013,36(1):5.[doi:1001-3938(2013)06-0005-07]

备注/Memo

备注/Memo:
收稿日期:2014-09-23
作者简介:柏明卓(1980—),男,硕士,工程师,主要从事管线钢产品开发和生产工艺研究工作。
更新日期/Last Update: