参考文献/References:
[1]ALCARAZ J L, GIL S J, MARTINEZ-ESNAOLA J M. A fracture condition based on the upper bound method for the extrusion of bimetallic tubes[J]. Journal of Materials Processing Technology, 1996, 61(3): 265-274.
[2]WRIGHT H, ODUYEMI T, EVANS H R. The experimental behaviour of double skin composite elements[J]. Journal of Constructional Steel Research,1991(19): 91 -110.[3]CHEN W C , PETERSEN C W. Corrosion performance of welded CRA-lined pipes for flow lines[J]. SPE Production Engineering ,1992, 7(4): 357-378.
[4]巢鹏飞,杨连发,于强,等. 塑性成形技术在金属复合管制备中的应用及展望[J]. 塑性工程学报,2005,12(2):42-47.
[5]刘富君,郑津洋,郭小联,等. 双层管液压胀合的原理及力学分析[J]. 机械强度,2006,28(1): 99-103.
[6]郭明海,刘俊友,庞于思,等. 双金属管复合技术的研究进展(上)[J]. 钢管,2013,42(1): 11-16.
[7]谷霞,张安义,秦建平,等. 双金属复合管塑性复合成形工艺及应用[J]. 精密成形工程,2011,3(3):46-50.
[8]陈明徽,蔡休刚. 国外双金属复合钢管生产概况[J]. 钢管,1997,26(6): 23-28.
[9]孙育禄,白真,张国超,等. 油气田防腐用双金属复合管研究现状[J]. 全面腐蚀控制,2011,25(5):10-13.[10] API 5LD—1998, Specification for CRA Clad or Lined Steel Pipe[S].
[11] SY /T 6623—2005,内覆或衬里耐腐蚀合金钢管[S].
[12] DNVOS-F101—2007, Submarine Pipeline Systems[S].
相似文献/References:
[1]虞毅,徐连勇,韩永典,等.X65/316L机械复合管焊接接头CO2腐蚀行为研究[J].焊管,2011,34(1):13.[doi:1001-3938(2011)01-0013-04]
[2]王永芳,袁江龙,张燕飞,等.双金属复合管的技术现状和发展方向[J].焊管,2013,36(2):5.[doi:1001-3938(2013)02-0005-05]
WANG Yongfang,YUAN Jianglong,ZHANG Yanfei,et al.Technology Status and Development Direction of Bimetal Pipe[J].,2013,36(12):5.[doi:1001-3938(2013)02-0005-05]
[3]吴星东,谢树军.X65/316L与AISI4130/Inconel625复合管焊接接头力学性能及腐蚀行为研究[J].焊管,2014,37(3):14.[doi:1001-3938(2014)03-0014-05]
WU Xingdong,XIE Shujun.Research on Mechanical Properties and Corrosion Behavior of Welded Joints of X65/316L and AISI4130/Inconel625 Clad Pipe[J].,2014,37(12):14.[doi:1001-3938(2014)03-0014-05]
[4]梁国萍,赵 欣,郭 霖,等.高强钢L485MB+316L双金属复合管对接焊工艺验证[J].焊管,2014,37(12):61.[doi:1001-3938(2014)12-0061-03]
LIANG Guoping,ZHAO Xin,GUO Lin,et al.Butt Welding Process Verification of High Strength Steel L485MB+316L Bimetal Composite Pipe[J].,2014,37(12):61.[doi:1001-3938(2014)12-0061-03]
[5]郑茂盛,帅 铭,钟雨心,等.表面状态对304不锈钢/20钢双金属复合管耐腐蚀性能的影响[J].焊管,2015,38(2):16.[doi:1001-3938(2015)02-0016-03]
ZHENG Maosheng,SHUAI Ming,ZHONG Yuxin,et al.Influence of Surface Status on Corrosion Resistance of Stainless Steel 304/20 Steel Bimetal Composite Pipe[J].,2015,38(12):16.[doi:1001-3938(2015)02-0016-03]
[6]张城举,李 霄,牛 辉,等.L415+316L机械复合管焊接接头失效分析[J].焊管,2016,39(2):1.[doi:10.19291/j.cnki.1001-3938.2016.02.001]
ZHANG Chengju,LI Xiao,NIU Hui,et al.Failure Analysis on Welded Joint of L415+316L Mechanical Composite Pipe[J].,2016,39(12):1.[doi:10.19291/j.cnki.1001-3938.2016.02.001]
[7]李良均,崔成武,蒋 勇,等.L415/N08825复合管硫化物应力腐蚀开裂及失重腐蚀研究[J].焊管,2017,40(2):6.[doi:10.19291/j.cnki.1001-3938.2017.02.002]
LI Liangjun,CUI Chengwu,JIANG Yong,et al.Study on Sulfide Stress Corrosion Cracking and Weight Loss Corrosion?of L415/N08825 Clad Pipe[J].,2017,40(12):6.[doi:10.19291/j.cnki.1001-3938.2017.02.002]
[8]任保剑,何 清,张付峰,等.N08825镍基合金复合管件加工技术及耐蚀性研究[J].焊管,2017,40(8):33.[doi:10.19291/j.cnki.1001-3938.2017.08.006]
REN Baojian,HE Qing,ZHANG Fufeng,et al.Study on N08825 Nickel Base Alloy Composite Pipe Fittings Processing Technology and Corrosion Resistance[J].,2017,40(12):33.[doi:10.19291/j.cnki.1001-3938.2017.08.006]
[9]梁国萍,王 斌,王敏瑞,等.内衬316L双金属复合管环焊焊缝失效原因分析[J].焊管,2017,40(9):34.[doi:10.19291/j.cnki.1001-3938.2017.09.008]
LIANG Guoping,WANG Bin,WANG Minrui,et al.Failure Reason Analysis on Butt Welds of Lined with 316L Bimetal Composite Pipe Butt Weld[J].,2017,40(12):34.[doi:10.19291/j.cnki.1001-3938.2017.09.008]