[1]徐腊梅,吴世杰,娄月霞,等.钢管无溶剂内减阻涂层的制备工艺研究[J].焊管,2018,41(5):44-47,52.[doi:10.19291/j.cnki.1001-3938.2018.05.008]
 XU Lamei,WU Shijie,LOU Yuexia,et al.Preparation Technology Research of Non-solvent Interior Friction-reduction Coating for Steel Pipe[J].,2018,41(5):44-47,52.[doi:10.19291/j.cnki.1001-3938.2018.05.008]
点击复制

钢管无溶剂内减阻涂层的制备工艺研究()
分享到:

《焊管》[ISSN:1001-3938/CN:61-1160/TE]

卷:
41
期数:
2018年第5期
页码:
44-47,52
栏目:
应用与开发
出版日期:
2018-05-28

文章信息/Info

Title:
Preparation Technology Research of
 Non-solvent Interior Friction-reduction Coating for Steel Pipe
文章编号:
10.19291/j.cnki.1001-3938.2018.05.008
作者:
徐腊梅吴世杰娄月霞 冯鹏霄
中石化石油机械股份有限公司沙市钢管分公司,湖北 荆州 434001
Author(s):
XU Lamei WU Shijie LOU Yuexia FENG Pengxiao
Shashi Steel Pipe Branch Company, Sinopec Petroleum Machinery Co., Ltd., Jingzhou 434001, Hubei, China
关键词:
钢管防腐内减阻涂层无溶剂环氧涂料防腐工艺
Keywords:
steel pipe anticorrosion friction-reduction coating non-solvent epoxy coating anticorrosion technology
分类号:
TE988
DOI:
10.19291/j.cnki.1001-3938.2018.05.008
文献标志码:
B
摘要:
为了获得钢管高质量的无溶剂环氧涂料内减阻涂层,通过对无溶剂环氧涂料的输送条件和内喷涂工艺原理的分析,设计了钢管无溶剂内减阻涂层的制备工艺。采用设计的制备工艺,对Φ1 219 mm和Φ1 016 mm钢管进行了无溶剂环氧涂料内减阻喷涂,并对涂层的质量和性能进行了检测。检测结果表明,采用该工艺制备的涂层的各项性能满足相关标准的要求。说明设计的内减阻涂层制备工艺合理,可用于Φ1 219 mm和Φ1 016 mm钢管的无溶剂环氧涂料内减阻喷涂。
Abstract:
In order to obtain high-quality non-solvent epoxy interior friction-reduction coating for steel pipe, by analyzing the conveying condition and inner spraying process principle of non-solvent epoxy coating, preparation technology of non-solvent interior friction-reduction coating for steel pipe was designed. The non-solvent interior friction-reduction spraying was taken on Φ1 219 mm and Φ1 016 mm steel pipes with the designed preparation technology, and the quality and performance of the coating were tested. The testing results showed that all the performances of the coating with the designed technology met relevant standards. It indicated that the designed interior friction-reduction coating preparation technology was reasonable and could be used for non-solvent epoxy interior friction-reduction spraying for Φ1 219 mm and Φ1 016 mm steel pipes.

参考文献/References:

[1] 杨继平,毛浓召,杜华,等. 输气管道内壁无溶剂内减阻环氧涂层的应用研究[J]. 焊管,2015,38(1):33-37.
[2] SPE-0000CC02,潜江-韶关输气管道工程采购文件无溶剂内减阻涂层[S].
[3] 徐振海. 无溶剂环氧涂料在大型储罐防腐中的应用[J]. 腐蚀研究,2017,31 (6):68-72.
[4] API RP 5L 2:2002,非腐蚀性气体输送用管线管内部涂层推荐作法 附录G[S].
[5] ASTM D4541:2009,Standard Test Method for Pull-off Strength of Coatings Using Portable Adhesion Testers[S].
[6] ISO 8503-4:2012,Preparation of Steel Substrates Before Application of Paints and Related Products-Surface Roughness Characteristics of Blast-cleaned Steel Substrates-Part 4:Method for the Calibration of ISO Surface Profile Comparators and for the Determination of Surface Profile-Stylus Instrument Procedure[S].
[7] 许大华,孙金海. 机械制造技术[M]. 北京:国防工业出版社,2015.
[8] 王志魁. 化工原理[M]. 北京:化学工业出版社,2010.
[9] 刘广文. 天然气管道内涂层减阻技术[M]. 北京:石油工业出版社,2001.

相似文献/References:

[1]李春林.条形码技术在钢管企业中的应用[J].焊管,2007,30(4):47.[doi:1001-3938(2007)04-0047-02]
 LI Chun-lin.Application of Bar Code Technology by Steel Pipe Enterprise[J].,2007,30(5):47.[doi:1001-3938(2007)04-0047-02]
[2]张朝生 编译.高强度管道钢管表面应力腐蚀裂纹的研究[J].焊管,2007,30(4):82.[doi:1001-3938(2007)04-0083-03]
 Edited and Translated by ZHANG Chao-sheng.Study on Surface Stress Corrosion Crack of High Strength Pipeline[J].,2007,30(5):82.[doi:1001-3938(2007)04-0083-03]
[3]孙 宏.高钢级螺旋缝焊接钢管拉伸试样类型选择[J].焊管,2007,30(5):36.[doi:1001-3938(2007)05-0036-03]
 SUN Hong.Study of Choosing the Tensile Test Specimen’s Type for High Grade SSAW Steel Pipe[J].,2007,30(5):36.[doi:1001-3938(2007)05-0036-03]
[4]任立元,任天翔,翁乐宁,等.管道防腐补口用热缩带固定片应力开裂探讨[J].焊管,2007,30(5):89.[doi:1001-3938(2007)05-0089-04]
 REN Li-yuan,REN Tian-xiang,WENG Le-ning,et al.Discussion on Stress Crack of Hot Shrinkalbe Belt Stator Used for Coating Repair of Pipeline[J].,2007,30(5):89.[doi:1001-3938(2007)05-0089-04]
[5]郭继富,王素娟,张艳龙,等.钢管数控仿形锯锯片TiAlN涂层技术的应用[J].焊管,2007,30(6):48.[doi:1001-3938(2007)06-0048-03]
 GUO Ji-fu,WANG Shu-juan,ZHANG Yan-long,et al.Application of TiAlN Coating Technology of Numerical Control and Profile Modeling Saw Chip for Steel Pipe[J].,2007,30(5):48.[doi:1001-3938(2007)06-0048-03]
[6]岳进才.常见钢管质量问题及成因分析[J].焊管,2008,31(1):64.[doi:1001-3938(2008)01-0064-06]
 YUE Jin-cai.Common Quality Problem & Cause Analyses of Steel Pipe[J].,2008,31(5):64.[doi:1001-3938(2008)01-0064-06]
[7]赵 坤.浅谈ERW钢管错边缺陷[J].焊管,2008,31(2):67.[doi:1001-3938(2008)02-0067-02]
 ZHAO Kun.Brief Discussion on Offset Defect of ERW Pipe[J].,2008,31(5):67.[doi:1001-3938(2008)02-0067-02]
[8]郭艳玲,高真凤,张兴虎.俄罗斯国内钢管产销趋势[J].焊管,2008,31(2):86.[doi:1001-3938(2008)02-0086-05]
 GUO Yan-ling,GAO Zhen-feng,ZHANG Xing-hu.Trends of Steel Pipe Production and Sale in Russia[J].,2008,31(5):86.[doi:1001-3938(2008)02-0086-05]
[9]张正龙.Φ219 mm钢管内涂层“缩坑”缺陷分析[J].焊管,2008,31(4):64.[doi:1001-3938(2008)04-0064-03]
 ZHANG Zheng-long.Analysis on ‘Shrinkage Dent’of Φ219 mm Steel Pipe Internal Coating[J].,2008,31(5):64.[doi:1001-3938(2008)04-0064-03]
[10]冯来义,罗晓梅.钢管预热中频设备可控硅的正确使用及保护[J].焊管,2008,31(5):66.[doi:1001-3938(2008)05-0066-04]
 FENG Lai-yi,LUO Xiao-mei.Corrective Using & Protecting of Silicon Controlled Rectifier in Intermediate Frequency Induction Heating Equipment[J].,2008,31(5):66.[doi:1001-3938(2008)05-0066-04]
[11]韩 勇,陈华栋,蒲旭亮.多管环氧粉末喷涂一次成型工艺及主要设备探讨[J].焊管,2013,36(7):42.[doi:1001-3938(2013)07-0042-04]
 HAN Yong,CHEN Huadong,PU Xuliang.Discussion on One-step Forming Process of Multitube Epoxy Powder Coating and Main Equipment[J].,2013,36(5):42.[doi:1001-3938(2013)07-0042-04]
[12]涂君俊.钢管外防腐主机模头烟尘净化系统的设计与应用[J].焊管,2014,37(2):38.[doi:1001-3938(2014)02-0038-03]
 TU Junjun.Design and Application of Smoke and Dust Purification System forSteel Pipe External Corrosion Host Head[J].,2014,37(5):38.[doi:1001-3938(2014)02-0038-03]
[13]鲍新愿,张 茜,贾 真,等.钢管防腐中频感应加热设备循环水冷系统的改进[J].焊管,2015,38(9):56.[doi:1001-3938(2015)09-0056-05]
 BAO Xinyuan,ZHANG Qian,JIA Zhen,et al.Circulating Water-cooling System Improvement of Steel Pipe Anticorrosion Medium Frequency Induction Heating Device[J].,2015,38(5):56.[doi:1001-3938(2015)09-0056-05]
[14]李 辉,王鹏起,周 权,等.钢质管道防腐用聚乙烯拉伸性能研究[J].焊管,2017,40(12):63.[doi:DOI: 10.19291/j.cnki.1001-3938.2017.12.014]
 LI Hui,WANG Pengqi,ZHOU Quan,et al.Research on Tensile Property of Polyethylene for Anti-corrosion of Steel Pipe[J].,2017,40(5):63.[doi:DOI: 10.19291/j.cnki.1001-3938.2017.12.014]
[15]惠林林.防腐生产线抛丸工艺对钢管外表面粗糙度的影响[J].焊管,2018,41(10):65.[doi:10.19291/j.cnki.1001-3938.2018.10.014]
 HUI Linlin.Discussion and Research on the Effect of Shot Blasting Process on the Surface Roughness of Steel Pipe[J].,2018,41(5):65.[doi:10.19291/j.cnki.1001-3938.2018.10.014]

备注/Memo

备注/Memo:

收稿日期:2017-11-23

作者简介:徐腊梅(1986—),女,湖北孝感人,工艺工程师,现主要从事油气管道防腐技术方面的工作。

更新日期/Last Update: 2018-05-28