[1]夏连宁,张 亮,李 琦,等.大直径输水钢管承插搭接焊接口设计与应用[J].焊管,2019,42(5):60-64.[doi:10.19291/j.cnki.1001-3938.2019.5.010]
 XIA Lianning,ZHANG Liang,LI Qi,et al.Design and Application of Socket Lap Welding Joint for Large Diameter Water Transmission Steel Pipe[J].,2019,42(5):60-64.[doi:10.19291/j.cnki.1001-3938.2019.5.010]
点击复制

大直径输水钢管承插搭接焊接口设计与应用()
分享到:

《焊管》[ISSN:1001-3938/CN:61-1160/TE]

卷:
42
期数:
2019年第5期
页码:
60-64
栏目:
经验交流
出版日期:
2019-05-28

文章信息/Info

Title:
Design and Application of Socket Lap Welding Joint
for Large Diameter Water Transmission Steel Pipe
文章编号:
10.19291/j.cnki.1001-3938.2019.5.010
作者:
夏连宁1张 亮2李 琦2明 皓2
1. 上海福谙管道技术有限公司, 上海 201203;
2. 山东禹王管业有限公司, 山东 邹平 256200
Author(s):
XIA Lianning1 ZHANG Liang2 LI Qi2 MING Hao2
1. Shanghai Fuan Pipe Tech Co., Ltd., Shanghai 201203, China;
2. Shandong Yuwang Pipe Industry Co., Ltd., Zouping 256200, Shandong, China
关键词:
输水钢管对接焊承插搭接焊大直径埋地管道角焊
Keywords:
water transmission steel pipe butt welding socket lap welding large diameter buried pipeline fillet welding
分类号:
TG441.2
DOI:
10.19291/j.cnki.1001-3938.2019.5.010
文献标志码:
B
摘要:
针对国内目前大直径输水钢管现场对接焊安装时出现的对接质量低、速度慢、焊接接口漏水等问题,结合国外应用经验,通过对承插搭接焊接口进行参数设计和受力分析,设计了一种大直径输水钢管承插焊连接方式,并通过试验模拟了现场焊接和试压。结果表明,钢管承插搭接焊连接可降低对接难度,提高对接速度和接口的密封性,以期为我国输水钢管的生产和安装提供更好的解决方案。
Abstract:
Aiming at the problems of low butt quality, slow speed and leakage of welding interface occurred in the field butt welding and installation of large diameter water transmission steel pipe in China, combined with foreign application experience, through the parameter design and force analysis of socket lap joint, a socket welding connection mode of large diameter water conveying pipe was designed, and field welding and pressure test were simulated by experiment. The test results showed that socket lap welding connection of steel pipe can reduce the difficulty of butt joint, improve the speed of butt joint and the tightness of the interface, and provide a better solution for the production and installation of water transmission steel pipe in China.

参考文献/References:

[1] 张玉先, 陈欣, 张硕, 等. 常州市大口径输水钢管爆管原因与对策研究[J]. 给水排水, 2006, 32(7): 89-93.
[2] 沈之基. 我国输水钢管同国外的差距及几点建议(四)——对国内某条输水钢管线的点评和再设计[J]. 焊管,  2007, 30(6): 15-18.
[3] 杨健. 大管径埋地管道承插焊连接施工技术[J]. 石油化工建设, 2006, 28(1): 54-56.
[4] 刘听移.大口径半球型承插式钢管施工技术及应用实例[J]. 给水排水, 2004, 30(10): 91-93.
[5] ASME BPVC VIII-1—2017, Rules for Construction of Pressure Vessels[S].
[6] ASME BPVC II-D—2015,Properties[S].
[7] 周质炎, 夏连宁. 埋地柔性钢管设计与结构分析[M]. 上海: 上海科学技术出版社, 2019.
[8] ANSI/AWWA C200—2017, Steel Water Pipe[S].
[9] BROCKENBROUGH R L. Strength of bell-and-spigot joints[J]. Journal of Structural Engineering, 1990, 116(7): 1983-1991.
[10] 夏连宁. 美标输水钢管设计、制造与安装[J]. 给水排水, 2015, 41(11): 86-91.

相似文献/References:

[1]沈之基.我国输水钢管同国外的差距及几点建议(三)——输水钢管管端接口技术[J].焊管,2007,30(4):18.[doi:1001-3938(2007)04-0018-03]
 SHEN Zhi-ji.Difference in Steel Pipe for Water Transmission Between Domestic and Abroad,and Some Suggestions(Ⅲ)——Technology of pipe end connection for water Transmission pipeline[J].,2007,30(5):18.[doi:1001-3938(2007)04-0018-03]
[2]尹长华,靳海成.大直径厚壁X70级钢管与绝缘接头基材P460NH管段的焊接[J].焊管,2007,30(4):36.[doi:1001-3938(2007)04-0036-05]
 YIN Chang-hua,JIN Hai-cheng.The Welding of Heavy-caliber Thick Wall X70 Steel Pipe and Insulated Rail Joint Parent Metal P460NH[J].,2007,30(5):36.[doi:1001-3938(2007)04-0036-05]
[3]左丽娜,张希川,刘忠仁,等.冰箱及空调用铜铝管焊接技术综述[J].焊管,2008,31(3):39.[doi:1001-3938(2008)03-0039-03]
 ZUO Li-na,ZHANG Xi-chuan,LIU Zhong-ren,et al.Welding Technology of Copper and Aluminum Pipe Used in Refrigerators and Air Conditions[J].,2008,31(5):39.[doi:1001-3938(2008)03-0039-03]
[4]周建宏,石 凯,卢雪峰,等.国产CT80级连续油管用钢带对接焊焊接方法探讨[J].焊管,2009,32(5):25.[doi:1001-3938(2009)05-0025-03]
 ZHOU Jian-hong,SHI Kai,LU Xue-feng,et al.Discussion on Strip Butt-welding Method of CT80 Grade Coiled Tubing Made in China[J].,2009,32(5):25.[doi:1001-3938(2009)05-0025-03]
[5]李霄,石凯,刘彦明,等.连续管焊接工艺及接头性能研究[J].焊管,2012,35(5):15.[doi:1001-3938(2012)05-0015-04]
 LI Xiao,SHI Kai,LIU Yan-ming,et al.Research on Coiled Tubing Butt Welding Process and Properties of Welded Joint[J].,2012,35(5):15.[doi:1001-3938(2012)05-0015-04]
[6]夏连宁.大直径钢管承插式连接在输水管道中的应用[J].焊管,2015,38(9):45.[doi:1001-3938(2015)09-0045-06]
 XIA Lianning.Application of Large Diameter Steel Pipe Spigot Joint in Water Pipeline[J].,2015,38(5):45.[doi:1001-3938(2015)09-0045-06]
[7]温庆伦,李 霄,姬二佳.连续油管对接焊残余应力场分析[J].焊管,2016,39(4):5.[doi:10.19291/j.cnki.1001-3938.2016.04.002]
 WEN Qinglun,LI Xiao,JI Erjia.Coiled Tubing Butt Welding Residual Stress Field Analysis[J].,2016,39(5):5.[doi:10.19291/j.cnki.1001-3938.2016.04.002]
[8]梁国萍,王 斌,王敏瑞,等.内衬316L双金属复合管环焊焊缝失效原因分析[J].焊管,2017,40(9):34.[doi:10.19291/j.cnki.1001-3938.2017.09.008]
 LIANG Guoping,WANG Bin,WANG Minrui,et al.Failure Reason Analysis on Butt Welds of Lined with 316L Bimetal Composite Pipe Butt Weld[J].,2017,40(5):34.[doi:10.19291/j.cnki.1001-3938.2017.09.008]
[9]张锦刚,等.石油钢管行业新型焊接技术应用与发展现状[J].焊管,2018,41(5):8.[doi:10.19291/j.cnki.1001-3938.2018.05.002]
 ZHANG Jingang,BI Zongyue,XU Xueli.Development Situation and Application of New Welding Technology in Petroleum and Steel Pipe Industry[J].,2018,41(5):8.[doi:10.19291/j.cnki.1001-3938.2018.05.002]
[10]王 斌,梁国萍,王小艳,等.焊接工艺对双金属复合管对接焊缝晶间腐蚀的影响[J].焊管,2018,41(6):47.[doi:10.19291/j.cnki.1001-3938.2018.06.011]
 WANG Bin,LIANG Guoping,WANG Xiaoyan,et al.Influence of Different Welding Processes on Intergranular Corrosion ofBimetal-lined Pipe Butt Weld[J].,2018,41(5):47.[doi:10.19291/j.cnki.1001-3938.2018.06.011]

备注/Memo

备注/Memo:

收稿日期:2019-01-14

作者简介:夏连宁(1961—),男,高级工程师,原美国西北管道公司顾问,美国ASCE和AWWA会员,现为上海福谙管道技术有限公司总经理,主要从事大直径输水管道结构设计、生产工艺研究和管道施工方法等方面的技术研究工作。

更新日期/Last Update: 2019-06-20