[1]鲜 宁,等.连续油管在酸性环境下的弯曲疲劳寿命研究[J].焊管,2020,43(1):15-19.[doi:10.19291/j.cnki.1001-3938.2020.01.003]
 XIAN Ning,JIANG Fang,et al.Research on the Bend Fatigue Life of the Coiled Tubing Exposed to Sour Environments[J].,2020,43(1):15-19.[doi:10.19291/j.cnki.1001-3938.2020.01.003]
点击复制

连续油管在酸性环境下的弯曲疲劳寿命研究()
分享到:

《焊管》[ISSN:1001-3938/CN:61-1160/TE]

卷:
43
期数:
2020年第1期
页码:
15-19
栏目:
试验与研究
出版日期:
2020-01-28

文章信息/Info

Title:
Research on the Bend Fatigue Life of the Coiled Tubing Exposed to Sour Environments
文章编号:
10.19291/j.cnki.1001-3938.2020.01.003
作者:
鲜 宁1 2姜 放1荣 明1 2张 平3邹先雄3崔 磊1 2
1. 中国石油集团管力学与环境重点实验室四川分室, 成都 610041;
 2. 中国石油工程建设公司西南分公司, 成都 610041;
 3. 中国石油川庆钻探工程公司, 成都 610051
Author(s):
XIAN Ning1 2 JIANG Fang1 RONG Ming1 2 ZHANG Ping3 ZOU Xianxiong3 CUI Lei1 2
1. Sichuan Research Division of CNPC Key Lab for Mechanical and Environment Behavior of Tubular Goods, Chengdu 610041,China;
2. China Petroleum Engineering & Construction Corp, Southwest company, Chengdu 610041,China;
3. CNPC Chuanqing Drilling Engineering Company Limited , Chengdu 610051,China
关键词:
连续油管弯曲腐蚀疲劳H2S
Keywords:
coiled tubing bend corrosion fatigue H2S
分类号:
TG174.3
DOI:
10.19291/j.cnki.1001-3938.2020.01.003
文献标志码:
A
摘要:
为了准确评价连续油管在酸性环境下的腐蚀疲劳寿命,对CT80钢级Φ38.1 mm×3.18 mm的连续油管管段在不同条件下进行了弯曲腐蚀疲劳试验。结果显示:经过酸性腐蚀环境的浸泡后,连续油管的弯曲疲劳寿命显著下降,约为大气环境下弯曲疲劳寿命的34.6%~45.2%,其平均值约为39.7%;对于未出现HIC的连续油管,在酸性腐蚀环境下起下不同井次后,连续油管的总疲劳寿命相近。连续油管经腐蚀浸泡取出在大气环境中放置24 h后,氢原子从连续油管管体溢出,塑性部分回升,约为大气环境下弯曲疲劳寿命的68.9%。
Abstract:
In order to accurately evaluate the corrosion fatigue life of the coiled tubing in acid environment,CT80 steel Φ38.1 mm×3.18 mm of the coiled tubing section bending corrosion fatigue tests have been carried out under different conditions. The results showed that the bending fatigue life of the coiled tubing decreased significantly after immersing in acid corrosion environment,which was about 34.6%~45.2% of the bending fatigue life in atmospheric environment, and the average value was about 39.7%. For the coiled tubing without HIC,the total fatigue life of the coiled tubing was similar after the different well runs in acid corrosion conditions. After the coiled tubing soaked in the corrosive solution is taken out and placed in the atmospheric environment for 24 hours,hydrogen atoms escaped from the coiled tubing body,and the plastic part recovered, approximately 68.9% of the bending fatigue life in the atmosphere.

参考文献/References:

[1] HAMPSON R, MOIR C, FREENEY T. Working with coiled tubing in H2S and CO2 wells[C]//Presented at the 2009 SPE/ICoTA Coiled Tubing and Well Intervention Conference and Exhibition. The Woodlands,TX,USA:A Global Perspective,SPE 12129431,2009.
[2] CRABTREE A R, GAVIN W. Coiled tubing in sour environments-theory and practice[C]//Presented at the 2004 SPE/ICoTA Coiled Tubing Conference and Exhibition. Houston,TX,USA:SPE 89614,2004.
[3] 鲜宁,姜放,荣明,等. 连续油管在酸性环境下的腐蚀与防护及其研究进展[J]. 天然气工业,2011,39(4):120-123.
[4] 王峻乔.连续油管技术分析与研究[J]. 石油矿场机械,2005,34(5):34-36.
[5] 鲜宁,姜放,施岱艳,等. H2S环境下碳钢连续油管的SSC行为研究[J]. 腐蚀与防护,2012,33(S2):142-145.
[6 ] 鲜宁,张平,荣明,等. 连续油管在酸性环境下的疲劳寿命研究进展[J]. 天然气与石油,2019,37(1):63-67.
[7] LARSEN H A, REICHERT B A. Coiled tubing abrasion-an experimental study of field failures[C]//Presented at the 2003 SPE/ICoTA Coiled Tubing Conference. Houston,TX,USA:SPE 81724,2003.
[8] STANLEY R K. An analysis of failure in coiled tubing[C]//IADC/SPE Drilling Conference. Dallas,TX,USA:IADC/SPE 39352,1998.
[9] WILLEM P, ADRICHEN V, LARSEN H A. Coiled tubing failure statistics used to develop CT performance indicators[C]//IADC/SPE Drilling Conference. Dallas,TX,USA:IADC/SPE 78808,2002.
[10] 李鸿斌,毕宗岳,余晗,等. Φ31.8连续油管断裂失效分析[J]. 焊管,2016,39(5):31-36.
[11] IWONA S O, NOWINKA J, WILDE G, et al. Coiled tubing performance evaluation for sour service under variable loading conditions[C]// NACE Corrosion 2001.Houston,TX,USA:NACE ,2001.
[12] HAMPSON R,MOIR C,FREENEY T. Working with coiled tubing in H2S and CO2 wells[C]//Presented at the 2009 SPE/ICoTA Coiled Tubing and Well Intervention Conference and Exhibition. The Woodlands,TX,USA:A Global Perspective,SPE 121294,2009.
[13] CRABTREE A R. CT-Failure monitoring: A decade of experience[C]//Presented at the 2008 SPE/ICoTA Coiled Tubing and Well Intervention Conference and Exhibition. The Woodlands,TX,USA:SPE 113676, 2008.
[14] HISHAM A. DIN N E, ARAMCO S, et al. Workovers in sour environments: how do we avoid coiled tubing failures[C]//Presented at the 2004 1st International Symposium Oilfield Corrosion. Aberdeen,USA: SPE 87622, 2004.
[15] LUFT H B. The low cycle fatigue and plastic strain response of coiled tubing in a sour environment without corrosion inhibitor protection[C]//Presented at the 2003 SPE/ICoTA Coiled Tubing Conference. Houston,TX,USA: SPE 81723,2003.
[16] PADRON T, LUFT B, KEE E. Fatigue life of coiled tubing with external mechanical damage[C]//Presented at the 2007 SPE/ICoTA Coiled Tubing and Well Intervention Conference and Exhibition. The Woodlands,TX,USA:SPE 107113,2007.
[17] PADRON T, DATAHAM G. Effect of external mechanical damage on the fatigue life of coiled tubing exposed to sour environments criteria for CT100 grade[C]//Presented at the 2009 SPE/ICoTA Coiled Tubing and Well Intervention Conference and Exhibition. The Woodlands,TX,USA:SPE 120827,2009.
[18] PADRON T. Sour serviceability of higher-strength coiled tubing final results[C]//Presented at the 2010 SPE/ICoTA Coiled Tubing and Well Intervention Conference and Exhibition.The Woodlands,TX,USA:SPE 130279,2010.
[19] PADRON T. Effect of external mechanical damage on the fatigue life of coiled tubing exposed to sour environments[C]// Presented at the 2008 SPE/ICoTA Coiled Tubing and Well Intervention Conference and Exhibition. The Woodlands,TX,USA: SPE 113149,2008.
[20] KENNETH R. Residual curvature and moments in CT due to bending[C]//Presented at the 2015 SPE/ICoTA Coiled Tubing and Well Intervention Conference and Exhibition. The Woodlands,TX,USA: SPE 173641-MS,2015.
[21] REICHERT B, NGUYEN T, ROLOVIC R. Advancements in fatigue testing and analysis[C]//Presented at the 2016 SPE/ICoTA Coiled Tubing and Well Intervention Conference and Exhibition. Houston,TX,USA:SPE 179064-MS,2016.

相似文献/References:

[1]周建宏,石 凯,卢雪峰,等.国产CT80级连续油管用钢带对接焊焊接方法探讨[J].焊管,2009,32(5):25.[doi:1001-3938(2009)05-0025-03]
 ZHOU Jian-hong,SHI Kai,LU Xue-feng,et al.Discussion on Strip Butt-welding Method of CT80 Grade Coiled Tubing Made in China[J].,2009,32(1):25.[doi:1001-3938(2009)05-0025-03]
[2]王文武,李继红,赵鹏康,等.连续油管环焊温度场及残余应力场数值分析[J].焊管,2011,34(3):18.
[3]秦跃平,张佃平.连续油管在油田洗井作业中的应用[J].焊管,2011,34(9):53.
[4]梁根选,金时麟 编译.连续油管下井作业技术与设备[J].焊管,2011,34(10):72.[doi:1001-3938(2011)10-0072-06]
 Edited and Translated by LIANG Gen-xuan,JIN Shi-lin.Coiled Tubing Technology and Equipment[J].,2011,34(1):72.[doi:1001-3938(2011)10-0072-06]
[5]李 琳,李继红,余 晗,等.连续油管TIG焊焊接接头最薄弱区工艺-性能神经网络预测模型[J].焊管,2012,35(1):5.[doi:1001-3938(2012)01-0005-03]
 LI Lin,LI Ji-hong,YU Han,et al.The Neural Network Prediction Model of Process-property in the Weakest Area of Coiled Tubing TIG Welded Joint[J].,2012,35(1):5.[doi:1001-3938(2012)01-0005-03]
[6]罗 鹏,秦跃平,陈 锐,等.体积压裂与速度管柱排液复合技术的应用[J].焊管,2012,35(1):29.[doi:1001-3938(2012)01-0029-04]
 LUO Peng,QIN Yue-ping,CHEN Rui,et al.Application of Volume Fracturing and Velocity String Discharging Fluid Composite Technology[J].,2012,35(1):29.[doi:1001-3938(2012)01-0029-04]
[7]李继红,李 琳,赵鹏康,等.连续油管直缝高频焊热影响区最薄弱区硬度的神经网络预测[J].焊管,2012,35(7):5.[doi:1001-3938(2012)07-0005-04]
 LI Ji-hong,LI Lin,ZHAO Peng-kang,et al.The Neural Network Prediction of Hardness in the Weakest Area of Coiled Tubing in HFW HAZ[J].,2012,35(1):5.[doi:1001-3938(2012)07-0005-04]
[8]毕宗岳.连续油管及其应用技术进展[J].焊管,2012,35(9):5.[doi:1001-3938(2012)09-0005-08]
 BI Zongyue.Coiled Tubing (CT) and Its Application Technology Development[J].,2012,35(1):5.[doi:1001-3938(2012)09-0005-08]
[9]冀亚锋,张 宏,毕宗岳,等.连续油管材料临界CTOD值计算方法研究[J].焊管,2012,35(11):5.[doi:001-3938(2012)11-0005-04]
 JI Yafeng,ZHANG Hong,BI Zongyue,et al.Research on a New Method for Calculating Critical CTOD Value of Coiled Tubing Material[J].,2012,35(1):5.[doi:001-3938(2012)11-0005-04]
[10]王新强,鲁明春,包俊清,等.连续油管氮气泡沫冲砂工艺在涩北气田的成功应用[J].焊管,2013,36(5):38.[doi:1001-3938(2013)05-0038-03]
 WANG Xinqiang,LU Mingchun,BAO Junqing,et al.Successful Application of Coiled Tubing Nitrogen Foam Sand Flushing Technology in China Sebei Gas Field[J].,2013,36(1):38.[doi:1001-3938(2013)05-0038-03]

备注/Memo

备注/Memo:
收稿日期:2019-09-04
基金项目: 国家863重大专项“大型油气田及煤层气开发”(项目编号2016 ZX 05023006-005)。
作者简介:鲜  宁(1980—),男,重庆市人,硕士,高级工程师,主要从事材料的腐蚀与防护技术研究。
更新日期/Last Update: 2020-02-21