[1]高欣蕊,黄流群,何 清,等.超大直径钢制弯管3PE全自动防腐设备的开发[J].焊管,2021,44(1):38-42.[doi:10.19291/j.cnki.1001-3938.2021.01.007]
 GAO Xinrui,HUANG Liuqun,HE Qing,et al.Development of 3PE Automatic Anti-corrosion Equipment for Extra-large Diameter Steel Bend Pipe[J].,2021,44(1):38-42.[doi:10.19291/j.cnki.1001-3938.2021.01.007]
点击复制

超大直径钢制弯管3PE全自动防腐设备的开发()
分享到:

《焊管》[ISSN:1001-3938/CN:61-1160/TE]

卷:
第44卷
期数:
2021年第1期
页码:
38-42
栏目:
工艺与设备
出版日期:
2021-01-28

文章信息/Info

Title:
Development of 3PE Automatic Anti-corrosion Equipment for Extra-large Diameter Steel Bend Pipe
文章编号:
10.19291/j.cnki.1001-3938.2021.01.007
作者:
高欣蕊黄流群何 清张付峰袁希海肖松节白 杨丁维娅
1. 郑州万达重工股份有限公司,郑州 450000;
2. 中国石油天然气管道工程有限公司,河北 廊坊065000
Author(s):
GAO Xinrui HUANG Liuqun HE Qing ZHANG FufengYUAN Xihai XIAO Songjie BAI Yang DING Weiya
1. Zhengzhou Wanda Heavy Co., Ltd., Zhengzhou 450000, China;
2. China Petroleum Pipeline Engineering Co., Ltd., Langfang 065000, Hebei, China
关键词:
自动化防腐超大直径钢制弯管环氧粉末防腐带聚乙烯带
Keywords:
automatic anticorrosion large diameter steel bend epoxy powder corrosion protection polyethylene adhesive tape
分类号:
TE988
DOI:
10.19291/j.cnki.1001-3938.2021.01.007
文献标志码:
B
摘要:
目前超大直径弯管的防腐作业主要采用手工操作,不仅效率低,生产成本高,而且生产过程对环境污染大。开发了一条超大直径钢制弯管自动化防腐生产线,把喷涂及自动缠带设计成一条生产线,将防腐带缠绕系统和环氧系统联动、合一,充分利用弯制余热,进行聚乙烯带缠带作业。检测结果表明,新设计的自动化防腐技术满足GB/T 23257—2017标准中超大直径弯管防腐层的要求,在防腐工艺上减少了原有预热工序,节约了能源,提高了效率,且生产过程绿色环保。
Abstract:
At present, the anti-corrosion operation of super large diameter elbow mainly adopts manual operation, which not only has low efficiency, high production cost, but also has great environmental pollution in the production process. An automatic anti-corrosion production line for super large diameter steel bend pipe is developed. The spraying and automatic tape winding are designed as a production line. The anti-corrosion tape winding system and epoxy system are linked and integrated into a fully automatic production line. The bended waste hea is fully utilized for polyethylene tape winding. The test results show that the newly designed automatic anti-corrosion technology meets the requirements of GB/T 23257—2017 standard for the anti-corrosion coating of super large diameter bend pipe, reduces the original preheating process in the anti-corrosion process, saves energy, improves the efficiency, and the production process is green and environment-protective.

参考文献/References:

[1] GB/T 8923.1―2011,涂覆涂料前钢材表面处理 表面清洁度的目视评定 第1部分:未涂覆过的钢材表面和全面清除原有涂层后的钢材表面的锈蚀等级和处理等级[S].

[2] GB/T 23257―2017,附录K:防腐层剥离强度测定方法[S].
[3] SY/T 0315―2013,钢质管道熔结环氧粉末外涂层技术规范[S].
[4] API SPEC 5L―2012,管线钢管规范[S].
[5] GB/T 985—2008,气焊、手工电弧焊及气体保护焊焊缝坡口的基本形式与尺寸[S].
[6] GB/T 18253—2018,钢及钢产品 检验文件的类型[S].
[7] 王湘鸣,章跃,周广宏,等. 医用不锈钢表面改性及腐蚀磨损研究进展[J]. 腐蚀科学与防护技术,2015,27(1):95-98.
[8] 施利炳. 金属的腐蚀与防护[J]. 物理测试,2003(3):41.
[9] 林海潮,李谋成. 涂层下金属的腐蚀过程[J]. 腐蚀科学与防护技术,2002,14(3):180-181.
[10] 吴荫顺. 腐蚀试验方法与防护检测技术[M]. 北京:化学工业出版社,1996.
[11] 曹楚南. 腐蚀电化学[M]. 北京:化学工业出版社,1994.
[12] 肖纪美. 腐蚀总论-材料的腐蚀剂及其控制方法[M]. 北京:化学工业出版社,1994.
[13] 刘永辉,张佩芬. 金属腐蚀学原理[M]. 北京:航空工业出版社,1993:20.
[14] 张宝宏,从文博. 金属电化学腐蚀与防护[M]. 北京:化学工业出版社,2005.

备注/Memo

备注/Memo:
收稿日期:2020-08-21
作者简介:高欣蕊(1987—),工程师,主要从事钢制管件的产品研发工作。
更新日期/Last Update: 2021-03-22