[1]刘炜辰,李嘉良,蒋浩泽 编译.日本第一条X80高强度管线钢管的设计制造与现场施工[J].焊管,2021,44(1):48.[doi:10.19291/j.cnki.1001-3938.2021.01.009]
 Translated by LIU Weichen,LI Jialiang,JIANG Haoze.Design Manufacture and Construction of the First X80 High Strength Steel Pipe in Japan[J].,2021,44(1):48.[doi:10.19291/j.cnki.1001-3938.2021.01.009]
点击复制

日本第一条X80高强度管线钢管的设计制造与现场施工()
分享到:

《焊管》[ISSN:1001-3938/CN:61-1160/TE]

卷:
第44卷
期数:
2021年第1期
页码:
48
栏目:
国外焊管
出版日期:
2021-01-28

文章信息/Info

Title:
Design Manufacture and Construction of the First X80 High Strength Steel Pipe in Japan
文章编号:
10.19291/j.cnki.1001-3938.2021.01.009
作者:
刘炜辰李嘉良蒋浩泽 编译
1. 中国石油测井公司国际事业部,北京 102206;
2. 成都索贝数码科技股份有限公司,成都 610041;
3. 中国石油测井公司,西安 710089
Author(s):
Translated by LIU Weichen LI Jialiang JIANG Haoze
1. International Business Department, China Petroleum Logging Co., Ltd., Beijing 102206, China;
2. Chengdu SOBEY Digital Technology Co., Ltd., Chengdu 610041, China;
3. China Petroleum Logging Co., Ltd., Xi’an 710089, China
关键词:
X80管线钢管道设计管线钢管环缝焊接
Keywords:
X80 pipeline steel piping design line pipe girth welding
分类号:
TG444.7
DOI:
10.19291/j.cnki.1001-3938.2021.01.009
文献标志码:
B
摘要:
为了全面了解日本第一条X80钢级高压输气管道工程的建设情况,从管道设计思路、管材制造、环缝焊接工艺及施工等方面进行了总结和分析。由于该管线安装在城市地区,设计要求具有极高的安全性和抗震性能。为了保证管道安全,将最大工作压力下的许用环向应力限制在222 MPa以下;工程用板材成分设计中严格控制Ti/N比,轧制采用了动态加速冷却技术,保证大批量高效生产的钢板满足钢管技术规范的要求;钢管采用了160 ℃的低温外涂层工艺,各项力学性能均超过了API标准的基本要求;环缝焊接采用与母材完全高强匹配的焊接材料,研发了性能和无损检测质量优良的机械GMAW焊接工艺。该管道各项技术可为高强度管道的建设提供借鉴。
Abstract:
In order to fully understand the construction situation of the first X80 steel grade high pressure gas transmission pipeline project in Japan, the pipeline design ideas, pipe material manufacturing, girth welding process and construction and other aspects are summarized and analyzed. It is found that the pipeline is installed in urban areas and the design requires high safety and seismic performance. In order to ensure pipeline safety, the allowable circumferential stress under the maximum working pressure should be limited below 222 MPa; Ti/N ratio is strictly controlled in the composition design of sheet metal used in engineering. New dynamic accelerated cooling is adopted in rolling to ensure that the steel plate produced in large quantities and efficiently meets the requirements of steel tube technical specifications. The steel pipe adopts the low-temperature external coating process at 160 °C, and the mechanical properties exceeded the basic requirements of API standard. The girth welding adopts the welding material that is fully matched with the base metal, and the mechanical GMAW welding process with excellent performance and NDI quality is developed. The technologies of this pipeline can provide reference for the construction of high-strength pipelines.

相似文献/References:

[1]孙宏.西气东输二线用国产X80钢级螺旋埋弧焊管性能分析[J].焊管,2010,33(2):13.[doi:1001-3938(2010)02-0013-04]
 SUN Hong.Analysis on Domestic X80 Grade SAWH Pipe Property Used in the[J].,2010,33(1):13.[doi:1001-3938(2010)02-0013-04]
[2]李立科,郑茂盛,孙利军,等.热处理对X80管线钢组织性能的影响[J].焊管,2010,33(4):18.[doi:1001-3938(2010)04-0018-04]
 LI Li-ke,ZHENG Mao-sheng,SUN Li-jun,et al.The Influence of Heat Treatment on Microstructure Properties of X80 Pipeline Steel[J].,2010,33(1):18.[doi:1001-3938(2010)04-0018-04]
[3]王娜,雷阿利.X80管线钢焊接接头中焊缝的耐蚀性的研究[J].焊管,2010,33(5):24.[doi:1001-3938(2010)05-0024-06]
 WANG Na,LEI A-li.Research on the Corrosion Restistance of X80 Pipeline Steel Welding Joints in Sulfer-containing Medium[J].,2010,33(1):24.[doi:1001-3938(2010)05-0024-06]
[4]张敏,赵鹏康,毕宗岳,等.X80管线钢用气体保护焊丝的研制[J].焊管,2010,33(10):23.[doi:1001-3938(2010)10-0023-06]
 ZHANG Min,ZHAO Peng-kang,BI Zong-yue,et al.Development of Gas-shielded Welding Wire for X80 Pipeline Steel[J].,2010,33(1):23.[doi:1001-3938(2010)10-0023-06]
[5]李根全,肖凡,李志忠,等.螺旋埋弧焊管焊缝韧性[J].焊管,2010,33(8):24.[doi:1001-3938(2010)08-0024-04]
 LI Gen-quan,XIAO Fan,LI Zhi-zhong,et al.Weld Toughness of SAWH Pipes[J].,2010,33(1):24.[doi:1001-3938(2010)08-0024-04]
[6]刘振伟,郭 晖,尚成嘉.高Nb X80管线钢的应变时效研究[J].焊管,2011,34(5):12.
[7]贾改风,梁永昌,王文录,等.邯钢厚规格X80管线钢的研发与应用[J].焊管,2011,34(11):24.[doi:1001-3938(2011)11-0024-06]
 JIA Gai-feng,LIANG Yong-chang,WANG Wen-lu,et al.Development and Application of X80 Pipeline Steel with Heavy Wall Thickness in HanSteel[J].,2011,34(1):24.[doi:1001-3938(2011)11-0024-06]
[8]赵志伟,徐 强,彭立山,等.X80感应加热弯管回火工艺研究[J].焊管,2012,35(1):44.[doi:1001-3938-(2012)01-0044-04]
 ZHAO Zhi-wei,XU Qiang,PENG Li-shan,et al.Study on Tempering Process of X80 Induction Heating Bend[J].,2012,35(1):44.[doi:1001-3938-(2012)01-0044-04]
[9]韩晨.高铌和低铌X80管线钢动态再结晶行为的研究[J].焊管,2012,35(2):10.[doi:1001-3938(2012)02-0010-06]
 HAN Chen.Study on Dynamic Recrystallization Behavior of High-Nb and Low-Nb X80 Pipeline Steel[J].,2012,35(1):10.[doi:1001-3938(2012)02-0010-06]
[10]韩秀林,李国鹏,张丽娜,等.X80直缝埋弧焊管制管前后拉伸性能的变化[J].焊管,2012,35(3):19.[doi:1001-3938(2012)03-0019-05]
 HAN Xiu-lin,LI Guo-peng,ZHANG li-na,et al.Study on the Tensile Property Before and After Forming of X80 SAWL Pipe[J].,2012,35(1):19.[doi:1001-3938(2012)03-0019-05]

备注/Memo

备注/Memo:
收稿日期:2020-07-13
作者简介:刘炜辰(1993—),男,硕士,工程师,现主要从事石油测井解释工作。
更新日期/Last Update: 2021-03-22