[1]顾华军,卜明哲,付现桥,等.盐穴储气库卤水介质对A3钢腐蚀规律研究及防护分析[J].焊管,2022,45(10):12-17.[doi:10.19291/j.cnki.1001-3938.2022.10.003]
 GU Huajun,BU Mingzhe,FU Xianqiao,et al.Corrosion Law Study and Protection Analysis of A3 Steel by Brine Medium in Salt Cave Gas Storage[J].,2022,45(10):12-17.[doi:10.19291/j.cnki.1001-3938.2022.10.003]
点击复制

盐穴储气库卤水介质对A3钢腐蚀规律研究及防护分析()
分享到:

《焊管》[ISSN:1001-3938/CN:61-1160/TE]

卷:
45
期数:
2022年第10期
页码:
12-17
栏目:
试验与研究
出版日期:
2022-10-28

文章信息/Info

Title:
Corrosion Law Study and Protection Analysis of A3 Steel by Brine Medium in Salt Cave Gas Storage
文章编号:
10.19291/j.cnki.1001-3938.2022.10.003
作者:
顾华军卜明哲付现桥刘瑞凯周晓光李 晔陈紫苑李子茂朱加祥
1. 中国石油工程建设有限公司, 北京 100120; 2. 中国石油大学(华东) 材料科学与工程学院,山东 青岛 266580; 3. 国家管网集团工程技术创新有限公司, 天津 300450; 4. 中国石油工程建设有限公司华北分公司, 河北 任丘 062550; 5. 济宁市特种设备检验研究院, 山东 济宁 272000
Author(s):
GU Huajun BU Mingzhe FU Xianqiao LIU Ruikai ZHOU Xiaoguang LI Ye CHEN Ziyuan LI Zimao ZHU Jiaxiang
1. China Petroleum Engineering & Construction Corporation, Beijing 100120, China; 2. School of Materials Science and Engineering, China University of Petroleum(East China), Qingdao 266580, Shandong, China; 3. PipeChina Engineering Technology Innovation Co., Ltd., Tianjin 300450, China; 4. North China Branch of Petro China Engineering Construction Corporation, Renqiu 062550, Hebei, China; 5. Jining Special Equipment Inspection Institute, Jining 272000, Shandong, China
关键词:
地下储气库卤水管道A3钢耐蚀性腐蚀速率
Keywords:
underground gas storage the brine pipes A3 steel corrosion resistance rate of corrosion
分类号:
GT172
DOI:
10.19291/j.cnki.1001-3938.2022.10.003
文献标志码:
A
摘要:
为了解决地下盐穴储气库注采管线与造腔管线合并带来的造腔期的卤水腐蚀问题,采用水腐蚀性测试方法,研究了地下盐穴储气库卤水管道工况和介质对管道腐蚀的影响规律。研究结果表明,温度、卤水浓度、溶解氧含量、流速均会加剧卤水对A3钢的腐蚀,结合卤水管道应用工况,建议选用双金属复合钢管,既能起到优良的耐蚀防护作用,又能在一定程度上降低成本,对实际工业生产具有较高的经济价值。
Abstract:
In order to solve the problem of brine corrosion in the cavity period caused by the merger of the underground salt cave gas storage pipeline and the cavity pipeline, the test method for corrosivity of water was used to study the effect of working condition and medium on corrosion of brine pipeline in underground salt cavern gas storage. The results show that temperature, brine concentration, dissolved oxygen content and flow rate will aggravate the corrosion of A3 steel by brine. Combined with the application conditions of brine pipeline, it is suggested to choose bimetallic composite steel pipe, which can not only play a good role in corrosion protection but also reduce the cost to a certain extent, and has high economic value for practical industrial production.

参考文献/References:

[1] 班凡生,高树生,单文文. 岩盐品位对岩盐储气库水溶建腔的影响[J]. 天然气工业,2006(4):115-118,164. [2] 江汉石油管理局勘察设计研究院. 水腐蚀性测试方法:SY/T 0026—1999[S]. 北京:石油工业出版社,1999. [3] 林学强,柳伟,张晶,等. 高温高压CO2/O2共存环境中TP100钢的腐蚀行为[J]. 腐蚀与防护,2013,34(8):698-701.[3] 胡建国,张志浩,孙银娟. 油田二氧化碳驱20#和L245NS管线钢腐蚀规律研究[J]. 油气田地面工程,2017,36(9):18-23.[4] OMAR I H,GUANLTUN Y M,KVAREKVAL J,et al. H2S corrosion of carbon steel under simulated Kashagan field conditions[C]//NACE International Corrosion/2005 Conference,Houston,US:NACE,2005:1-16.[5] 中国石油集团工程设计有限责任公司西南分公司. 钢质管道内腐蚀控制规范:GB/T 23258—2020[S]. 北京:中国标准出版社,2020.[6] 马晓红,孙锐艳,丛延刚,等. 含CO2气田不锈钢内衬复合钢管的选择及应用[J]. 石油规划设计,2013,24(2):18-21,48.[7] 李建中. 利用岩盐层建设盐穴地下储气库[J]. 天然气工业,2004(9):119-121,16.[8] 白海涛,王永清,马云,等. 温度对 CO2/盐水中碳钢腐蚀形貌的影响及其描述方法研究[J].表面技术,2018,47(8):204-210.[9] 岳昕. 国内外地下储气库安全管理及技术综述[J]. 当代化工,2017,46(5):921-924.[10] 徐敬,石光平,付现桥,等. 储气库注气管道选用研究[J]. 当代化工,2015,44(5):1152-1154,1157 .[11] 王美玲,胡莹,张志浩,等. 20碳钢在模拟油田水中的流动促进腐蚀行为[J]. 材料热处理学报,2018,39(12):84-90.[12] 谢飞,王丹,吴明,等. 溶解氧对X80管线钢腐蚀行为的影响及其机制[J]. 钢铁研究学报,2015,27(3):60-64.[13] 伍远辉,罗宿星,张显群,等. 氯离子含量对黄壤土中碳钢腐蚀行为的影响[J]. 全面腐蚀控制,2011,25(5):41-45.[14] 程小路,张波,程小辉,等. 天然气管道腐蚀与防护技术分析[J]. 科技经济导刊,2018(12):59.[15] 冉莉娜,完颜祺琪,王立献,等. 国外盐穴地下储气库发展趋势及启示[J]. 盐科学与化工,2017,46(12):9-12.

备注/Memo

备注/Memo:
收稿日期:2022-07-01
基金项目: 中国石油工程建设有限公司科技基金项目“储气库完整性分析研究”(项目编号CPECC2018KJ06285);中国石油工程建设有限公司科技基金项目“盐穴储气库再识别分析研究”(项目编号CPECC2019KJ09)。
作者简介:顾华军(1982—),男,硕士,工程师,主要从事储气库设计研究工作。