[1]田永强,何石磊,晁利宁,等.API J55套管腐蚀损伤剩余强度研究[J].焊管,2021,44(6):61-68.[doi:10.19291/j.cnki.1001-3938.2021.06.012]
 Translated by TIAN Yongqiang,HE Shilei,CHAO Lining,et al.Residual Strength of API J55 Casing Corrosion Damage[J].,2021,44(6):61-68.[doi:10.19291/j.cnki.1001-3938.2021.06.012]
点击复制

API J55套管腐蚀损伤剩余强度研究()
分享到:

《焊管》[ISSN:1001-3938/CN:61-1160/TE]

卷:
第44卷
期数:
2021年第6期
页码:
61-68
栏目:
国外焊管
出版日期:
2021-06-28

文章信息/Info

Title:
Residual Strength of API J55 Casing Corrosion Damage
文章编号:
10.19291/j.cnki.1001-3938.2021.06.012
作者:
田永强何石磊晁利宁李远征郭克星 ?编译
1. 国家石油天然气管材工程技术研究中心,陕西 宝鸡721008;
2. 宝鸡石油钢管有限责任公司,陕西 宝鸡721008
Author(s):
Translated by TIAN Yongqiang HE Shilei CHAO Lining LI Yuanzheng GUO Kexing
1. Chinese National Engineering Research Center for Petroleum and Natural Gas Tubular Goods, Baoji 721008,Shaanxi, China;?div>2. Baoji Petroleum Steel Pipe Co., Ltd., Baoji 721008, Shaanxi, China
关键词:
套管腐蚀缺陷剩余强度最大允许压力有限元分析
Keywords:
casing corrosion defect residual strength maximum allowed pressure finite element analysis
分类号:
TG174
DOI:
10.19291/j.cnki.1001-3938.2021.06.012
文献标志码:
A
摘要:
为了准确评估腐蚀损伤后的 API J55级HFW套管剩余强度,以在石油钻机中使用了70 000 h的套管为研究对象,通过加工不同损伤程度的人工缺陷对管道进行压力试验,研究了套管腐蚀损伤后管道内的最大允许压力评估标准,并进行了有限元数值模拟。采用ASME B31G标准、修订后的ASME B31G标准、CHoi’s 结论的三种表达式估算了腐蚀损伤后管道的剩余强度值,并与有限元分析结果进行了比较。结果表明,腐蚀损伤缺陷的深度小于管体的50%时,不会影响其结构的完整性;有限元模拟计算结果与试验结果吻合;利用有限元方法进行腐蚀损伤预测时很大程度上取决于其参考应力值。
Abstract:
In order to accurately evaluate the residual strength of API J55 HFW casing after corrosion damage, the casing used in oil drilling rig for 70 000 h was taken as the research object, and the pipeline pressure test was carried out by processing artificial defects with different damages. The maximum allowable pressure evaluation standard in the pipeline after corrosion damage was studied, and the finite element numerical simulation was carried out. The residual strength of the pipeline after corrosion damage is estimated by three formulas of ASME B31G standard, revised ASME B31G standard and CHoi’s conclusion, and compared with the results of finite element analysis. The results show that when the depth of corrosion damage defect is less than 50% of the pipe body, the structural integrity will not be affected. The results of finite element analysis simulation are in good agreement with the experimental results. When using the finite element method to predict the corrosion damage, it largely depends on the reference stress.

参考文献/References:

译自:SEDMAK A, Arsi■ M, ?譒arko■evi■ ?譕, et al. Remaining strength of API J55 steel casing pipes damaged by corrosion[J]. International Journal of Pressure Vessels and Piping, 2020(188): 104230.

相似文献/References:

[1]舒安庆,王韦华,魏化中.含腐蚀缺陷燃气管道极限载荷的有限元分析[J].焊管,2008,31(3):14.[doi:1001-3938(2008)03-0014-03]
 SHU An-qing,WANG Wei-hua,WEI Hua-zhong.Finite Element Analysis on Limit Load of Fuel Gas Pipelines with Corrosion Defects[J].,2008,31(6):14.[doi:1001-3938(2008)03-0014-03]
[2]蔡晓闻,高连新.我国油套管特殊螺纹接头的发展现状[J].焊管,2008,31(4):41.
 CAI Xiao-wen,GAO Lian-xin.Current Development Situation of the Special Thread Connection for Tubing/Casing[J].,2008,31(6):41.
[3]法 炜,李瑞涛.套管月牙形磨损程度预测研究进展[J].焊管,2009,32(3):20.[doi:1001-3938(2009)03-0020-03]
 FA Wei,LI Rui-tao.The Study of Evolution Casing Wear Degree Predicting[J].,2009,32(6):20.[doi:1001-3938(2009)03-0020-03]
[4]王绪华.套管钻井技术发展与应用[J].焊管,2009,32(10):33.[doi:1001-3938(2009)10-0033-04]
 WANG Xu-hua.The Development and Application of Casing Drilling Technology[J].,2009,32(6):33.[doi:1001-3938(2009)10-0033-04]
[5]申昭熙,赵建新,历建爱,等.全尺寸外压挤毁试验“异常”结果分析[J].焊管,2010,33(11):62.[doi:1001-3938(2010)11-0062-03]
[6]靖立君,闫光龙,赵文轸,等.动态与静态腐蚀电化学噪声特征的对比[J].焊管,2011,34(8):9.
[7]肖国章,高 霞,管磊磊,等.某油井套管腐蚀原因分析[J].焊管,2011,34(8):43.
[8]白 鹤,何石磊,党 涛,等.我国油套管特殊螺纹接头研究现状分析[J].焊管,2011,34(11):30.[doi:1001-3938(2011)11-0030-05]
 BAI He,HE Shi-lei,DANG Tao,et al.The Analysis of Research Status on China Domestic Tubing and Casing Premium Connection[J].,2011,34(6):30.[doi:1001-3938(2011)11-0030-05]
[9]史宏德,田青超,丁维军.N80钢级HFW套管的研发[J].焊管,2012,35(3):24.[doi:1001-3938(2012)03-0024-05]
 SHI Hong-de,TIAN Qing-chao,DING Wei-jun.Development of N80 Grade HFW Casing[J].,2012,35(6):24.[doi:1001-3938(2012)03-0024-05]
[10]李周波,毕宗岳,张 峰,等.Q125钢级SEW石油套管的研发[J].焊管,2013,36(8):32.[doi:1001-3938(2013)08-0004-32]
 LI Zhoubo,BI Zongyue,ZHANG Feng,et al.Research and Development of Q125 Grade SEW Oil Casing[J].,2013,36(6):32.[doi:1001-3938(2013)08-0004-32]

备注/Memo

备注/Memo:
收稿日期:2020-01-12
作者简介:田永强(1994—), 硕士,助理工程师,现主要从事油井管产品研究与开发工作。

更新日期/Last Update: 2021-07-06