[1]胡美娟,闵希华,罗金恒,等.凸台焊接对HFW焊管性能的影响[J].焊管,2018,41(3):53-57.[doi:10.19291/j.cnki.1001-3938.2018.03.011]
 HU Meijuan,MIN Xihua,LUO Jinheng,et al.Influence of Boss-backing Welding on HFW Pipe[J].,2018,41(3):53-57.[doi:10.19291/j.cnki.1001-3938.2018.03.011]
点击复制

凸台焊接对HFW焊管性能的影响()
分享到:

《焊管》[ISSN:1001-3938/CN:61-1160/TE]

卷:
41
期数:
2018年第3期
页码:
53-57
栏目:
经验交流
出版日期:
2018-03-28

文章信息/Info

Title:
Influence of Boss-backing Welding on HFW Pipe
文章编号:
10.19291/j.cnki.1001-3938.2018.03.011
作者:
胡美娟1闵希华2罗金恒1邵春明2张 杰2
1. 中国石油集团石油管工程技术研究院,西安 710077;
2. 中石油管道联合有限公司西部分公司, 乌鲁木齐 830013
Author(s):
HU Meijuan 1 MIN Xihua 2 LUO Jinheng 1 SHAO Chunming 2 ZHANG Jie 2
1. Tubular Goods Research center of CNPC, Xi’an 710077, China;
2. Petro China West Pipeline Company, Urumchi 830013, China
关键词:
站场阀室HFW焊管凸台交叉焊缝焊接残余应力微观组织
Keywords:
station and valve chamber HFW pipe boss-backing cross weld welding residual stress microstructure
分类号:
TE973
DOI:
10.19291/j.cnki.1001-3938.2018.03.011
文献标志码:
B
摘要:
为解决阀门、仪表和法兰等安装过程中凸台焊机位置不当对HFW焊管整体性能影响的问题,研究了凸台直接焊接对HFW焊管原始残余应力、微观组织的影响。研究表明,HFW电阻焊管上整体残余应力值较小,直焊缝区域残余应力值低于管体区域;凸台焊接后,交叉焊缝附近直焊缝上的轴向和管体上环向残余应力值陡增了2.5和3.8倍,分别为444 MPa和433 MPa;凸台焊接对HFW焊管上表面的侵入宽度为15.167 mm,厚度为3.376 mm,侵入区域出现了链状贝氏体。综上所述,建议在凸台焊接时采用较小的焊接热输入。
Abstract:
In order to solve the influence of unsuitable location of boss-backing welding on overall performance of HFW pipe during valve, instrument and flange Installation, the influence of boss-backing welding on the residual stresses and microstructure of HFW pipe were studied. The results showed that the overall residual stresses of HFW pipe were relatively low. The Residual stress at the longitudinal weld region were lower than the pipe body region. After the boss-backing welding, the axial residual stress at the longitudinal weld and the hoop residual stress at the pipe body region near the cross weld were increased sharply to 2.5 and 3.8 times, respectively, they were 444 MPa and 433 MPa. The invaded width to the HFW pipe after welding was about 15.167 mm, and the depth was about 3.376 mm, and there was chain-typed bainite in invaded zone. It was suggested that small welding heat input was adopted for boss-backing welding.

参考文献/References:

[1] 郭顺显. 管座在石化装置中的应用[J]. 石油化工设计, 1995, 12(4): 57-58.
[2] 谌贵宇, 郭艳林, 李巧, 等. 国内油气管道设计中小口径支管连接处理方式及发展趋势[J]. 天然气与石油, 2006, 24(4): 12-14.
[3] CHOI Y H, CHOI S Y. Assessment of socket weld integrity in pipings[J]. Journal of Loss Prevention in the Process Industries, 2009(22): 850-853.
[4] USA MSS, SP-97. Integrally reinforced forged branch outlet fittings-socket welding, treaded and butt welding Ends[S].
[5] 修俊杰. 小支管插套焊高周疲劳失效机理与延寿技术研究[D]. 天津:天津大学, 2012.
[6] SY4203—2007, 石油天然气建设工程施工质量验收规范-站内工艺管道工程[S].
[7] 吴雪峰. 交叉焊缝焊接残余应力对圆管相贯节点受力的影响[D]. 重庆大学, 2010.
[8] YOONJIN H, SANGHOON K, JEONGHO L, et al. Improvement of toughness of API X65 HFW pipe welds[C]// Proceedings of the 7th International Pipeline Conference. Calgary, Alberta, Canada, IPC2008-64233.
[9] JOACHIM K, HOLGER B, CHRISTOPH B. Influence of residual stress on the HIC resistance of high frequency induction welded pipes with regard to process-specific influencing factors[C]//Proceedings of the 8th International Pipeline Conference. Calgary, Alberta, Canada, IPC2010-31257.
[10] 张曙华. 残余应力对HFW管线管制造过程的影响分析[J]. 钢管, 2007, 36(6): 25-28.
[11] JAMES M N. Residual stress influences on structural reliability[J]. Engineering Failure Analysis, 2011, 18(8): 1909-1920.
[12] WAN X L, WANG H H, CHENG L, et al. The formation mechanisms of interlocked microstructures in low-carbon high-strength steel weld metals[J]. Materials Characterization, 2012, 67(3): 41-51.
[13] 焦程, 赵建平, 王鹏, 等. 锻制嵌入式支管座结构应力分析及优化设计[J]. 管道技术与设备, 2014(2): 5-7, 13.
[14] 胡美娟, 王鹏, 韩新利, 等. X80级抗大变形管线钢焊接粗晶区的组织和性能[J]. 焊接学报, 2012, 33(9): 93-96.
[15] GUNGOR O E, YAN P, THIBAUX P. Investigations into the microstructure-toughness relation in high frequency induction welded pipes[C]//Proceedings of the 8th International Pipeline Conference.Calgary, Alberta,Canada, IPC2010-31372.

相似文献/References:

[1]张 喆,周月明,白云峰,等.HFW中频热处理线圈结构对加热效果的影响[J].焊管,2009,32(1):41.[doi:1001-3938(2009)01-0041-05]
 ZHANG Zhe,ZHOU Yue-ming,BAI Yun-feng,et al.Loop Structure of HFW Intermediate Frequency Heating Treatment Effect to Heating[J].,2009,32(3):41.[doi:1001-3938(2009)01-0041-05]
[2]季晓鹏,张浩,马会文.国内外大中直径HFW焊管工艺发展研究[J].焊管,2009,32(8):10.[doi:1001-3938(2009)08-0010-06]
 JI Xiao-peng,ZHANG Hao,MA Hui-wen.Discussion on the Development and Research of the Technology of Large Diameter Hi-quality HFW Pipe in Abroad and Domestic[J].,2009,32(3):10.[doi:1001-3938(2009)08-0010-06]
[3]王涛.HFW焊管生产N80Q、P110级套管和油管的工艺开发[J].焊管,2009,32(9):35.[doi:1001-3938(2009)09-0035-03]
 WANG Tao.Process Development of HFW N80Q,P110 Grade Casing and Tubing[J].,2009,32(3):35.[doi:1001-3938(2009)09-0035-03]
[4]邵毅.ERW钢管内毛刺清除设备分析[J].焊管,2009,32(9):44.[doi:1001-3938(2009)09-0044-03]
 SHAO Yi.Inside Burrs Clearing Equipment Analysis of HFW Steel Pipe[J].,2009,32(3):44.[doi:1001-3938(2009)09-0044-03]
[5]邵毅.HFW焊管内毛刺清除刀具的选用[J].焊管,2009,32(12):40.[doi:1001-3938(2009)12-0040-03]
 SHAO Yi.Inside Burr Elimination Scraper Selection for HFW Pipe[J].,2009,32(3):40.[doi:1001-3938(2009)12-0040-03]
[6]孙凤龙,戴学余,周玉林,等.宝钢HFW焊管生产线去内毛刺刀杆研制[J].焊管,2010,33(1):37.[doi:1001-3938(2010)01-0037-04]
 SUN Feng-long,DAI Xue-yu,ZHOU Yu-lin,et al.Development of Scraper Bar for Burr Wiped off of HFW Pipe Line of Baosteel[J].,2010,33(3):37.[doi:1001-3938(2010)01-0037-04]
[7]彭在美.从国产连续油管成功研制看我国焊管产品结构调整[J].焊管,2010,33(4):5.[doi:1001-3938(2010)04-0005-05]
 PENG Zai-mei.Analyzing Structure Adjustment of China Welded Pipe Product from Successful Trial-production of Domestic Coiled Tubing[J].,2010,33(3):5.[doi:1001-3938(2010)04-0005-05]
[8]肖国章,高霞,李六五.带钢质量对ERW焊管质量的影响[J].焊管,2010,33(4):55.[doi:1001-3938(2010)04-0055-03]
 XIAO Guo-zhang,GAO Xia,LI Liu-wu.The Quality Of ERW Pipe Impacted By Strip Quality[J].,2010,33(3):55.[doi:1001-3938(2010)04-0055-03]
[9]张永,马东利.HFW焊管生产线乳化液回收泵站的改进[J].焊管,2010,33(6):45.[doi:1001-3938(2010)06-0045-02]
 ZHANG Yong,MA Dong-li.Emulsion Recycling Pump Station Alteration of HFW Production Line[J].,2010,33(3):45.[doi:1001-3938(2010)06-0045-02]
[10]赖兴涛,崔俊.HFW焊管制管各工序质量控制[J].焊管,2010,33(10):60.[doi:1001-3938(2010)10-0060-05]
 LAI Xing-tao,CUI Jun.Quality Control of HFW Pipe Each Procedure During Production[J].,2010,33(3):60.[doi:1001-3938(2010)10-0060-05]

备注/Memo

备注/Memo:

收稿日期: 2017-09-19

作者简介: 胡美娟(1981—),女,高级工程师,2009年毕业于西北工业大学,现从事石油管焊接工作。