[1]杨 明,刘玉卿,高 琦,等.西四线变壁厚钢管环焊缝内坡口设计方案[J].焊管,2021,44(3):11-16.[doi:10.19291/j.cnki.1001-3938.2021.03.003]
 YANG Ming,LIU Yuqing,GAO Qi,et al.Design Scheme of Inner Groove of Unequal Wall?span>Thickness Steel Pipe Girth Weld in the West-east Natural Gas Transmission IV[J].,2021,44(3):11-16.[doi:10.19291/j.cnki.1001-3938.2021.03.003]
点击复制

西四线变壁厚钢管环焊缝内坡口设计方案()
分享到:

《焊管》[ISSN:1001-3938/CN:61-1160/TE]

卷:
第44卷
期数:
2021年第3期
页码:
11-16
栏目:
应用与开发
出版日期:
2021-03-28

文章信息/Info

Title:
Design Scheme of Inner Groove of Unequal Wall?span>Thickness Steel Pipe Girth Weld in the West-east Natural Gas Transmission IV
文章编号:
10.19291/j.cnki.1001-3938.2021.03.003
作者:
杨 明刘玉卿高 琦张振永王慧庆
1. 国家管网集团西部管道有限责任公司,乌鲁木齐 830000;
2. 中国石油天然气管道工程有限公司,河北 廊坊 065000
Author(s):
YANG Ming LIU Yuqing GAO Qi ZHANG Zhenyong WANG Huiqing
1. Petrochina West Pipeline Company, Urumqi 830000, China;
2. China Petroleum Pipeline Engineering Corporation, Langfang 065000, Hebei, China
关键词:
油气管道变壁厚环焊缝锥孔型内坡口应力集中
Keywords:
oil and gas pipelines unequal wall thickness girth weld counterbore-tapered inner groove stress concentration
分类号:
TG441.3
DOI:
10.19291/j.cnki.1001-3938.2021.03.003
文献标志码:
A
摘要:
我国近些年发生多起油气管道环焊缝失效事故,其中超过半数的失效事故发生于变壁厚环焊缝上。针对变壁厚钢管环焊缝凸显的应力集中、焊接质量较差等问题,通过调研国内外相关行业先进经验和工程案例,提出了变壁厚钢管环焊缝锥孔型内坡口改进方案。以西四线(吐鲁番—中卫段)Φ1 422mm天然气管道工程为依托,基于焊接、无损检测、内检测、应力集中等要求,研究、改进了直管与直管变壁厚对接的环焊缝坡口型式,为提高变壁厚钢管环焊缝的焊接质量、提升管道本质安全提供了技术支持。
Abstract:
In recent years, failure of girth welds in oil and gas pipelines is common, and more than half of the failure accidents occurred in transition weld of unequal wall thickness. In order to solve the problem of stress concentration and poor welding quality in the unequal wall thickness girth weld, through the investigation of advanced experience and engineering cases of related industries at home and abroad, the counterbore-tapered inner groove of unequal wall thickness are proposed. Relying on the west-east natural gas transmission IV (Turpan-Zhongwei), based on welding, nondestructive testing, processing, internal inspection and stress concentration, a counterbore-tapered girth weld for joining straight pipes is designed, which provides technical support for improving the welding quality and the service reliability in oil and gas pipeline.

参考文献/References:

[1] 张宏,刘啸奔. 地质灾害作用下油气管道设计应变计算模型[J]. 油气储运,2017,36(1):91-97.

[2] 国务院安全委员会. 国务院安委会办公室关于贵州省黔西南州晴隆县“7·2”中石油输气管道燃烧爆炸事故的通报[EB/OL]. (2017-07-11)[2019-02-11]. http://www.chinasafety.gov.cn/awhsy/awhdt/201707/t20170711_2
13056.shtml.
[3] 应急管理部. 应急管理部组织召开油气管道安全生产警示会[EB/OL]. (2018-06-21)[2019-02-11]. http://www.
chinasafety.gov.cn/xw/bbgz/201806/t20180621_217077.
shtml.
[4] 张圣柱,程玉峰,冯晓东,等. X80管线钢性能特征及技术挑战[J]. 油气储运,2019,38(5):481-495.
[5] 罗金恒,杨锋平,王珂,等. 油气管道失效频率及失效案例分析[C]//2015年全国失效分析学术会议. 北京:[s.n.],2015:470-474.
[6] 张振永. 高钢级大口径天然气管道环焊缝安全提升设计关键[J]. 油气储运,2020,39(7):740-748.
[7] 张良,张广利,杨锋平,等. 环焊缝开裂原因分析[J]. 金属热处理,2014,39(12):151-156.
[8] HUO X T,KENNY S,HUSSEIN A,et al. Evaluation of back-beveled and counter bore-tapered joints in energy pipelines[C]//8th International Pipeline Conference. Calgary,Canada:IPC,2010:IPC2016-64390.
[9] DEKHANE A,LIU M,MARTENS M. Minimum counter bore length and tapered angle criteria for transition welds[C]//International Pipeline Conference. Calgary. Canada:IPC,2010: IPC2016-64614.
[10] MARTENS M,CHEN Y S,LIU M. Comparative integrity evaluation of counterbore-tapered and back-beveled weld joint[C]// International Pipeline Conference. Calgary,Canada:IPC,2014: IPC2014-33374.
[11] KYUBA H,DONG P. Equilibrium-equivalent structural stress approach to fatigue analysis of a tubular joint[J]. International Journal of Fatigue,2005,27(1):95-94.
[12] DONG P,HONG J K,CAO Z . Stresses and stress intensities at notches: ‘anomalous crack growth’ revisited[J]. International Journal of Fatigue,2003,25(9):811-825.
[13] DONG P,HONG J K,OSAGE D. Fatigue of piping and vessel welds: ASME’s FSRF rules revisited[C]//Proceedings of International Conference on Pressure Vessel and Piping. Vancouver,Canada:2002.
[14] NIEMI E. Stress determination for fatigue analyses of welded components[M]. Cambridge: Abington Publishing,1995.

相似文献/References:

[1]张振永,郭 彬.腐蚀管道剩余强度的确定及改造措施[J].焊管,2007,30(4):75.[doi:1001-3938(2007)04-0075-04]
 ZHANG Zhen-yong,GUO Bin.Determination of Residual Strength for Corrosion Pipeline and Rebuild Measures[J].,2007,30(3):75.[doi:1001-3938(2007)04-0075-04]
[2]徐庆磊,周 巍,尤海英,等.油气管道完整性管理体系分析[J].焊管,2007,30(6):81.[doi:1001-3938(2007)06-0081-04]
 XU QING-lei,LIU Ying,YOU Hai-ying,et al.Oil and Gas Pipeline Integrity Management System Analysis[J].,2007,30(3):81.[doi:1001-3938(2007)06-0081-04]
[3]刘 颖,刘长林,周 巍.油气管道的风险评价方法[J].焊管,2008,31(1):36.[doi:1001-3938(2008)01-0036-04]
 LIU Ying,LIU Chang-ling,ZHOU Wei.Risk Assessment of Oil-gas Pipeline[J].,2008,31(3):36.[doi:1001-3938(2008)01-0036-04]
[4]李为卫.油气输送管道用大直径双层埋弧焊管[J].焊管,2009,32(3):27.[doi:1001-3938(2009)03-0027-04]
 LI Wei-wei.Large Diameter& Double Layer SAW Linepipe for Oil and Gas[J].,2009,32(3):27.[doi:1001-3938(2009)03-0027-04]
[5]覃海涛,王爱民.管道补焊强度有限元分析[J].焊管,2009,32(7):22.[doi:1001-3938(2009)07-0022-04]
 QIN Hai-tao,WANG Ai-min.Finite Element Analysis of Repair Welding Strength in Oil Pipeline[J].,2009,32(3):22.[doi:1001-3938(2009)07-0022-04]
[6]薛振奎,隋永莉.焊接新技术在我国管道建设中的应用[J].焊管,2010,33(4):58.[doi:1001-3938(2010)04-0058-04]
 XUE Zhen-kui,SUI Yong-li.The Application of the New Welding Technology in Our Country Pipeline Construction[J].,2010,33(3):58.[doi:1001-3938(2010)04-0058-04]
[7]吉建立,许 勇,黄 龙,等.国内外油气管道防腐层阴极剥离试验方法及标准对比[J].焊管,2013,36(10):68.[doi:1001-3938(2013)10-0068-05]
 JI Jianli,XU Yong,HUANG Long,et al.Comparison of Cathodic Disbondment(CD) Test Methods andCriteria Between Overseas and China Oil and Gas Pipeline[J].,2013,36(3):68.[doi:1001-3938(2013)10-0068-05]
[8]郑茂盛,滕海鹏,胡 军,等.灰色理论用于油气管道安全性评价值得注意的问题[J].焊管,2013,36(11):20.[doi:1001-3938(2013)11-0020-03]
 ZHENG Maosheng,TENG Haipeng,HU Jun,et al.Notable Problems of Grey Theory Used in Safety Evaluation of Oil and Gas Pipeline[J].,2013,36(3):20.[doi:1001-3938(2013)11-0020-03]
[9]隋永莉,曹晓军,胡小坡.油气管道环焊缝焊接施工应关注的问题及建议[J].焊管,2014,37(5):62.[doi:1001-3938(2014)05-0062-04]
 SUI Yongli,CAO Xiaojun,HU Xiaopo.Focus on Problems and Suggestions of Oil and Gas Pipeline Circumferential Weld Welding at Site Construction[J].,2014,37(3):62.[doi:1001-3938(2014)05-0062-04]
[10]王国丽,庞艳风,谭建辉,等.油气管道全尺寸气体爆破试验场方案探讨[J].焊管,2015,38(4):33.[doi:1001-3938(2015)04-0033-05]
 WANG Guoli,PANG Yanfeng,TAN Jianhui,et al.Discussion on Full-size Gas Burst Test Field Used for Oil and Gas Pipeline[J].,2015,38(3):33.[doi:1001-3938(2015)04-0033-05]

备注/Memo

备注/Memo:
收稿日期:2020-12-07
作者简介:杨 明(1985—),男,高级工程师,从事输油气工艺相关技术研究工作。
更新日期/Last Update: 2021-05-07