[1]张国栋,白学军,李 颖,等.低温环境用厚壁大管径X80直缝埋弧焊管宽厚板的开发[J].焊管,2014,37(2):29-32.[doi:1001-3938(2014)02-0029-04]
 ZHANG Guodong,BAI Xuejun,LI Ying,et al.Development of Heavy Gauge Large Diameter X80 Pipeline Steel Platefor Low Temperature Environment Application[J].,2014,37(2):29-32.[doi:1001-3938(2014)02-0029-04]
点击复制

低温环境用厚壁大管径X80直缝埋弧焊管宽厚板的开发
分享到:

《焊管》[ISSN:1001-3938/CN:61-1160/TE]

卷:
37
期数:
2014年第2期
页码:
29-32
栏目:
应用与开发
出版日期:
2014-02-28

文章信息/Info

Title:
Development of Heavy Gauge Large Diameter X80 Pipeline Steel Plate
for Low Temperature Environment Application
文章编号:
1001-3938(2014)02-0029-04
作者:
张国栋1白学军1李 颖2谌铁强1王根矶1李 群1
(1. 秦皇岛首秦金属材料有限公司,河北 秦皇岛 066326;
2. 中油宝世顺(秦皇岛)有限公司,河北 秦皇岛066206)
Author(s):
ZHANG Guodong1 BAI Xuejun1 LI Ying2 CHEN Tieqiang1 WANG Genji1 LI Qun1
(1. Qinhuangdao Shouqin Metal Materials Co., Ltd., Qinhuangdao 066326,Heibei,China;
2. Zhongyou BSS (Qinhuangdao) Petropipe Co., Ltd.,Qinhuangdao 066326,Heibei,China)
关键词:
X80钢焊管大壁厚大管径低温韧性
Keywords:
X80 grade steel welded pipe heavy gauge large diameter low temperature
分类号:
TG115
DOI:
1001-3938(2014)02-0029-04
文献标志码:
A
摘要:
根据中亚天然气管道工程C线压气站用直缝管线钢管的技术条件,采用合理的成分设计、严格的炼钢质量控制及控轧控冷工艺,成功开发出具有良好低温韧性的X80宽厚板。产品微观组织以细小均匀的贝氏体为主,复合第二相弥散均匀分布的M/A组元。钢板具有高强度、低屈强比、优良的低温韧性和止裂韧性,在制管焊接过程中表现出良好的焊接性能,经过合理的JCOE工艺制成的直缝埋弧焊管成功应用于中亚C线压气站管线工程。
Abstract:
According to the technical specifications of the plate for compressor station of the third line of KAZAKHSTAN-CHINA Main Gas Pipeline(The Middle Asia C Line).The heavy gauge X80 wide plate with excellent toughness was developed by adopting reasonable composion design, strict steelmaking quality control and TMCP. A fine granular bainite+M/A constituents were obtained. The plates possess high strength, low Y/T ratio, high toughness, good low temperature crack arrest properties and weldability. The pipe produced with JCOE process was applied to the compressor station of The Middle Asia C Line project.

参考文献/References:

[1] API SPEC 5L, Specification for Line Pipe(44th edition)[S].
[2] ZAJAC S, SCHWINN V, TACKE K H. Characterisation and Quantification of Complex Bainitic Microstructures in High and Ultra-high Strength Linepipe Steels[J].Material Science Forum,2005,500-501:387-394.
[3] SUIKKANEN P, KARJALAINEN L, DEARDO A. Effect of Carbon Content on the Phase Transformation Characteristics, Microstructure and Properties of 500 MPa Grade Microalloyed Steels with Non-polygonal Ferrite Microstructures[J].La Metallurgia Italiana, 2008(05): 41-54. [4] REGIER R W, SPEER J G., MATLOCK D K, et al. Effect of Cooling Rate on the Crystallographic Effective Grain Size of Ferrite in Low-carbon Microalloyed Steels[C]∥Association for Iron and Steel Technology International Symposium on the Recent Developments in Plate Steels, Winter Park: [s.n.],2011: 351-363.
[5] KOSTRYZHEV A G, STRANGWOOD M, DAVIS C L. Bauschinger Effect in Microalloyed Steels: Part II. Influence of Work Softening on Strength Development during UOE Line-pipe Forming[J].Metallurgical and Materials Transactions A, 2011,42(10):3170-3177.
[6] SCHWINN V, FLUESS P, LIESSEM A, et al. Concepts of Grade X100 for High Toughness and Strain Based Design Application[C]∥Proceedings of the Eighteenth(2008)International Offshore and Polar Engineering Conference, Vancouver,Canada:[s.n.],2009:6-11.

[7] BIAN Y, PENNISTON C, COLLINS L, et al. Evaluation
of UOE and Spiral-welding Line Pipe for Strain-based Designs[C]∥Proceedings of the 8th International Pipeline Conference,Calgary: [s.n.],2010:139-148.
[8] DOUG STALHEIM. Metallurgical Optimization of Microalloyed Steels for Oil and Gas Transmission Pipelines[C]∥Proceedings and Presentation at the 6th International Conference on High Strength Low Alloy Steels(HSLA Steels 2011).Beijing: [s.n.],2011.
[9] API RP 5L3―1996, Recommended Practice for Conducting Drop-weight Tear Tests on Line Pipe 3rd Edition[S].
[10]KOSTRYZHEV A G,STRANGWOOD M,DAVIS C L. Bauschinger Effect in Microalloyed Steels:Part I.Depen-
dence on Dislocation-particle Interaction[J].Metallurgical and Materials Transactions A,2010,41(6):1399-1408.

相似文献/References:

[1]马海君.强力焊管的孔型设计[J].焊管,2007,30(4):56.[doi:1001-3938(2007)04-0056-02]
 MA Hai-jun.Pass Design of High-strength Welded Pipe[J].,2007,30(2):56.[doi:1001-3938(2007)04-0056-02]
[2]刘庆才,李 东,黎剑锋.影响输气管线钢管抗H2S性能主要因素的探讨[J].焊管,2007,30(5):54.[doi:1001-3938(2007)05-0054-05]
 LIU Qing-cai,LI Dong,LI Jian-feng.Key Factors Affecting Sour Service Ability of Welded Pipe and Its Domestic Production[J].,2007,30(2):54.[doi:1001-3938(2007)05-0054-05]
[3]彭在美.我国焊接钢管的发展进入重要的战略转折期[J].焊管,2008,31(6):5.[doi:1001-3938(2008)06-0005-10]
 PENG Zai-mei.The Development of China Welded Pipe Steps into the Important Strategic Transition Period[J].,2008,31(2):5.[doi:1001-3938(2008)06-0005-10]
[4]李霄,熊庆人,石凯,等.焊管残余应力研究进展及展望[J].焊管,2009,32(7):12.[doi:1001-3938(2009)07-0012-06]
 LI Xiao,XIONG Qing-ren,SHI Kai,et al.Research Progress and Prospect of Residual Stress in Welded Pipe[J].,2009,32(2):12.[doi:1001-3938(2009)07-0012-06]
[5]马 露 涛.φ720mm焊管平头机夹管装置设计[J].焊管,2009,32(9):47.[doi:1001-3938(2009)09-0047-03]
 MA Lu-tao.Design for φ720mm Welded Pipe Beveling Machine Clamp Pipe Device[J].,2009,32(2):47.[doi:1001-3938(2009)09-0047-03]
[6]耿开博.铝管、不锈钢管的高频感应焊接[J].焊管,2009,32(11):29.[doi:1001-3938(2009)11-0029-03]
 GENG Kai-bo.High-frequency Induction Welding of Aluminum and Stainless Steel Pipes[J].,2009,32(2):29.[doi:1001-3938(2009)11-0029-03]
[7]陈志翔,Jean Paul Boillot,Jeff Noruk.数字激光视觉技术在焊管生产中的应用[J].焊管,2010,33(2):29.[doi:1001-3938(2010)02-0029-04]
 CHEN Zhi-xiang,Jean Paul Boillot,Jeff Noruk.Application of Digital Laser Vision Technology in Welded Pipe Production[J].,2010,33(2):29.[doi:1001-3938(2010)02-0029-04]
[8]李珂,王自信,丁成飞.X80螺旋埋弧焊管管体强度影响因素分析[J].焊管,2010,33(4):22.[doi:1001-3938(2010)04-0022-04]
 LI Ke,WANG Zi-xin,DING Cheng-fei.Effect Factor Analysis on X80 SAWH Pipe Body Strength[J].,2010,33(2):22.[doi:1001-3938(2010)04-0022-04]
[9]郑茂盛,李立科,赵 青,等.热处理工艺对X80管线钢耐腐蚀性能的影响[J].焊管,2010,33(11):12.[doi:1001-3938(2010)11-0012-06]
 ZHENG Mao-sheng,LI Li-ke,ZHAO Qing,et al.Influence of Heat Treatment on Corrosive Resistance of X80 Pipeline Steel[J].,2010,33(2):12.[doi:1001-3938(2010)11-0012-06]
[10]黄克坚,苏章卓,甘遂谋,等.焊管机械扩径力的计算[J].焊管,2010,33(12):13.[doi:1001-3938(2010)12-0023-04]
[11]毕宗岳,牛爱军,牛 辉,等.国内外X80深水钻井隔水管主管性能对比[J].焊管,2013,36(11):5.[doi:1001-3938(2013)11-0005-05]
 BI Zongyue,NIU Aijun,NIU Hui,et al.Performance Comparison of Main Pipeline of X80 Deepwater Drilling Riser in Domestic and Overseas[J].,2013,36(2):5.[doi:1001-3938(2013)11-0005-05]
[12]刘振伟,王志太,孙志刚,等.高温预回火对X80螺旋埋弧焊管性能的影响[J].焊管,2015,38(11):20.[doi:1001-3938(2015)11-0020-06]
 LIU Zhenwei,WANG Zhitai,SUN Zhigang,et al.Influence of High-temperature Pre-tempering on X80 SAWH Pipe Performance[J].,2015,38(2):20.[doi:1001-3938(2015)11-0020-06]
[13]嵇 峰,张婷婷,吕成秀,等.X80钢级Φ1 219 mm×33 mm/37.9 mm热煨弯管研制[J].焊管,2019,42(1):17.[doi:10.19291/j.cnki.1001-3938.2019.1.003]
 JI Feng,ZHANG Tingting,LYU Chengxiu,et al.Development of X80 Φ1 219 mm×33 mm/37.9 mm Hot Induction Bend Pipe[J].,2019,42(2):17.[doi:10.19291/j.cnki.1001-3938.2019.1.003]

备注/Memo

备注/Memo:
收稿日期:2012-11-25
作者简介:张国栋(1984—),男,工程师,主要从事能源用钢的开发。
更新日期/Last Update: